Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ |
Abmessung
Property | Value | Comment |
---|---|---|
Breite | 205 - 800 mm Show Supplier Material materials with Breite of 205 - 800 mm | |
Dicke | 800 mm Show Supplier Material materials with Dicke of 800 mm | max. |
Durchmesser | 20 - 800 mm Show Supplier Material materials with Durchmesser of 20 - 800 mm | |
Länge | 2000 - 5800 mm Show Supplier Material materials with Länge of 2000 - 5800 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 12 % Show Supplier Material materials with Dehnung of 12 % | |
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa | Typical for Steels |
Härte, Brinell | 23.0 °C | 217 [-] Show Supplier Material materials with Härte, Brinell of 217 [-] | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Supplier Material materials with Poissonzahl of 0.29 [-] | Typical for Steels |
Streckgrenze | 23.0 °C | 550 MPa Show Supplier Material materials with Streckgrenze of 550 MPa | |
Zugfestigkeit | 23.0 °C | 1080 MPa Show Supplier Material materials with Zugfestigkeit of 1080 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.22E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.22E-5 1/K |
Wärmeleitfähigkeit | 23.0 °C | 42.6 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 42.6 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Chrom | 0.8 - 1.1 % Show Supplier Material materials with Chrom of 0.8 - 1.1 % |
Eisen | Balance |
Kohlenstoff | 0.4 - 0.45 % Show Supplier Material materials with Kohlenstoff of 0.4 - 0.45 % |
Mangan | 0.75 - 1 % Show Supplier Material materials with Mangan of 0.75 - 1 % |
Molybdän | 0.15 - 0.25 % Show Supplier Material materials with Molybdän of 0.15 - 0.25 % |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % |
Schwefel | 0.04 % Show Supplier Material materials with Schwefel of 0.04 % |
Silizium | 0.15 - 0.35 % Show Supplier Material materials with Silizium of 0.15 - 0.35 % |