Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ |
Abmessung
Property | Value | Comment |
---|---|---|
Breite | 205 - 800 mm Show Supplier Material materials with Breite of 205 - 800 mm | |
Dicke | 800 mm Show Supplier Material materials with Dicke of 800 mm | max. |
Durchmesser | 20 - 800 mm Show Supplier Material materials with Durchmesser of 20 - 800 mm | |
Länge | 2000 - 5800 mm Show Supplier Material materials with Länge of 2000 - 5800 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 12 % Show Supplier Material materials with Dehnung of 12 % | |
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa | Typical for Steels |
Härte, Brinell | 23.0 °C | 269 [-] Show Supplier Material materials with Härte, Brinell of 269 [-] | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Supplier Material materials with Poissonzahl of 0.29 [-] | Typical for Steels |
Streckgrenze | 23.0 °C | 835 MPa Show Supplier Material materials with Streckgrenze of 835 MPa | |
Zugfestigkeit | 23.0 °C | 980 MPa Show Supplier Material materials with Zugfestigkeit of 980 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.2E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.2E-5 1/K |
Spezifische Wärmekapazität | 23.0 °C | 450 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 450 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 44.5 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 44.5 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 2.48E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 2.48E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Chrom | 0.7 - 0.9 % Show Supplier Material materials with Chrom of 0.7 - 0.9 % |
Eisen | Balance |
Kohlenstoff | 0.38 - 0.43 % Show Supplier Material materials with Kohlenstoff of 0.38 - 0.43 % |
Mangan | 0.6 - 0.8 % Show Supplier Material materials with Mangan of 0.6 - 0.8 % |
Molybdän | 0.2 - 0.3 % Show Supplier Material materials with Molybdän of 0.2 - 0.3 % |
Nickel | 1.65 - 2 % Show Supplier Material materials with Nickel of 1.65 - 2 % |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % |
Schwefel | 0.04 % Show Supplier Material materials with Schwefel of 0.04 % |
Silizium | 0.15 - 0.35 % Show Supplier Material materials with Silizium of 0.15 - 0.35 % |