Abmessung
Property | Value | Comment |
---|---|---|
Breite | 205 - 800 mm Show Supplier Material materials with Breite of 205 - 800 mm | |
Dicke | 800 mm Show Supplier Material materials with Dicke of 800 mm | max. |
Durchmesser | 20 - 800 mm Show Supplier Material materials with Durchmesser of 20 - 800 mm | |
Länge | 3000 - 5800 mm Show Supplier Material materials with Länge of 3000 - 5800 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa | Typical for Steels |
Härte, Brinell | 23.0 °C | 197 - 241 [-] Show Supplier Material materials with Härte, Brinell of 197 - 241 [-] | Annealed |
Härte, Rockwell C | 23.0 °C | 60 - 62 [-] Show Supplier Material materials with Härte, Rockwell C of 60 - 62 [-] | Hardened |
Chemical properties
Property | Value |
---|---|
Chrom | 0.5 - 0.7 % Show Supplier Material materials with Chrom of 0.5 - 0.7 % |
Eisen | Balance |
Kohlenstoff | 0.9 - 1.05 % Show Supplier Material materials with Kohlenstoff of 0.9 - 1.05 % |
Mangan | 1 - 1.2 % Show Supplier Material materials with Mangan of 1 - 1.2 % |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % |
Silizium | 0.15 - 0.35 % Show Supplier Material materials with Silizium of 0.15 - 0.35 % |
Vanadium | 0.05 - 0.15 % Show Supplier Material materials with Vanadium of 0.05 - 0.15 % |
Wolfram | 0.5 - 0.7 % Show Supplier Material materials with Wolfram of 0.5 - 0.7 % |