Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa | Typical for Steels | ||
Härte, Rockwell C | 23.0 °C | 47 - 49 [-] Show Supplier Material materials with Härte, Rockwell C of 47 - 49 [-] | Tempered | ||
Härte, Brinell | Annealed |
Chemical properties
Property | Value |
---|---|
Chrom | 4.75 - 5.5 % Show Supplier Material materials with Chrom of 4.75 - 5.5 % |
Eisen | Balance |
Kohlenstoff | 0.45 % Show Supplier Material materials with Kohlenstoff of 0.45 % |
Mangan | 0.2 - 0.5 % Show Supplier Material materials with Mangan of 0.2 - 0.5 % |
Molybdän | 1.1 - 1.75 % Show Supplier Material materials with Molybdän of 1.1 - 1.75 % |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % |
Silizium | 0.8 - 1.2 % Show Supplier Material materials with Silizium of 0.8 - 1.2 % |
Vanadium | 0.9 - 1.1 % Show Supplier Material materials with Vanadium of 0.9 - 1.1 % |