Abmessung
Property | Value | Comment |
---|---|---|
Breite | 205 - 800 mm Show Supplier Material materials with Breite of 205 - 800 mm | |
Dicke | 800 mm Show Supplier Material materials with Dicke of 800 mm | max. |
Durchmesser | 20 - 800 mm Show Supplier Material materials with Durchmesser of 20 - 800 mm | |
Länge | 300 - 5800 mm Show Supplier Material materials with Länge of 300 - 5800 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa | Typical for Steels |
Härte, Brinell | 23.0 °C | 241 [-] Show Supplier Material materials with Härte, Brinell of 241 [-] | Annealed |
Härte, Rockwell C | 23.0 °C | 53 [-] Show Supplier Material materials with Härte, Rockwell C of 53 [-] | Hardened and Tempered |
Chemical properties
Property | Value |
---|---|
Chrom | 2.2 - 2.7 % Show Supplier Material materials with Chrom of 2.2 - 2.7 % |
Eisen | Balance |
Kohlenstoff | 0.3 - 0.4 % Show Supplier Material materials with Kohlenstoff of 0.3 - 0.4 % |
Mangan | 0.4 % Show Supplier Material materials with Mangan of 0.4 % |
Nickel | 1.4 - 1.8 % Show Supplier Material materials with Nickel of 1.4 - 1.8 % |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % |
Silizium | 0.4 % Show Supplier Material materials with Silizium of 0.4 % |
Vanadium | 0.2 - 0.5 % Show Supplier Material materials with Vanadium of 0.2 - 0.5 % |
Wolfram | 7.5 - 9 % Show Supplier Material materials with Wolfram of 7.5 - 9 % |