Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materialien
Categories
Sie sind nicht angemeldet
Categories
Metalllieferanten finden
List Your Company
Case Studies
Tools
Über uns
SAE 1006 HILUMIN® Ultra-clean nickel-plated
Tata Steel’s HILUMIN® is an electrolytically nickel-plated, diffusion-annealed cold-rolled steel strip. Manufactured using an ultra-clean steel grade, it plays an integral part in the production of batteries.
Diese Materialdaten wurden von TATA Steel zur Verfügung gestellt
All categories
Mechanische Systeme
Industriemaschinen
Verbindungselemente
Fasteners General
Luft- und Raumfahrt
Befestigungselemente für die Luft- und Raumfahrt
Schrauben
Schrauben
Scheiben
Nieten
Clamps & Staples
Lager
Bearings General
Shafts & Couplings
Other Shafts & Couplings
Federn
Automobil
Straßenfahrzeugsysteme
Übertragungen
Elektromotoren
Elektronik
Elektronische Komponenten
Motoren
Herstellung
Werkzeugmaschinensysteme
Other Machine Tool Systems
Bearbeitung
Sonstige Werkzeugmaschinen
Spanlose Arbeitsausrüstung
Schmiedepressen
Walzen
Extruding & Drawing Equipment
Walzausrüstung
Gussausrüstung
Gießformen
Other Chipless Working Equipment
Schweißen und Löten
Oberflächenbearbeitung und -beschichtung
Metallbeschichtungen
Bonding
Diffusion Bonding
Energie
Batterien
Battery Contacts
Solid State Batteries
Battery Anode
Battery Cathode
Battery Electrolyte
Solid State Electrolyte
Lithium-Ion Batteries
Elektrotechnik
Komponenten für Elektrogeräte
Other Components For Electrical Equipment
Allgemeine Fahrzeugteile
Braking System
Road Vehicles
Nutzfahrzeuge
Commercial Vehicles In General
Elektrofahrzeuge
Metallurgie
Iron & Steel Products
Steel Pipes & Tubes
Bau
Installationen in Gebäuden
Rohrleitungen
Konsumgüter
Haushaltselektrogeräte
General Appliances
Sportausrüstung und -einrichtungen
Sportausrüstung
Chemical properties
Property | Value | Comment |
---|---|---|
Kohlenstoff | 0.08 % Show Supplier Material materials with Kohlenstoff of 0.08 % | max. |
Mangan | 0.25 - 0.4 % Show Supplier Material materials with Mangan of 0.25 - 0.4 % | |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % | max. |
Schwefel | 0.05 % Show Supplier Material materials with Schwefel of 0.05 % | max. |
Technological properties
Property | ||||||||||||||||||||||||||||||||||||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Application areas | Battery components: cans, covers, connector strips | |||||||||||||||||||||||||||||||||||||||||||
Other |
| |||||||||||||||||||||||||||||||||||||||||||
Packaging size |
| |||||||||||||||||||||||||||||||||||||||||||
Surface Finish | ||||||||||||||||||||||||||||||||||||||||||||
Surface protection |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
UNTERNEHMEN
KONTAKTIEREN SIE UNS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.