Allgemein
Property | Value | Comment |
---|---|---|
Schichtnummer | 1.0 - 2.0 [-] Show Supplier Material materials with Schichtnummer of 1.0 - 2.0 [-] | Predominantly few-layer with some mono-layer and bi-layer |
Seitliche Flockengröße | 5000.0 Show Supplier Material materials with Seitliche Flockengröße of 5000.0 | Using SEM |
Mechanisch
Property | Value |
---|---|
Elastizitätsmodul | 1000.0 GPa Show Supplier Material materials with Elastizitätsmodul of 1000.0 GPa |
Thermisch
Property | Value |
---|---|
Wärmeleitfähigkeit | 1700 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 1700 W/(m·K) |
2000 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 2000 W/(m·K) |
Elektrisch
Property | Value |
---|---|
Bandabstand | 6.0 eV Show Supplier Material materials with Bandabstand of 6.0 eV |
Chemical properties
Property | Value |
---|---|
Bor | 40.0 - 44.0 % Show Supplier Material materials with Bor of 40.0 - 44.0 % |
Kohlenstoff | 6.0 - 10.0 % Show Supplier Material materials with Kohlenstoff of 6.0 - 10.0 % |
Sauerstoff | 2.0 - 4.0 % Show Supplier Material materials with Sauerstoff of 2.0 - 4.0 % |
Stickstoff | 43.0 - 47.0 % Show Supplier Material materials with Stickstoff of 43.0 - 47.0 % |
Technological properties
Property | ||
---|---|---|
Application areas | The lamellar structure of h-BN offers exceptional benefits as an additive in lubricants, and the high thermal conductivity and electrically insulating properties have promoted its use as a high performance additive for specialist lubricants, particularly where heat removal and electrical insulation are paramount. h-BN can be included in ceramics, alloys, resins, plastics and rubbers to improve insulating ability. Electronics, oxygen sensors, xerographic processes and laser printing. Proton conductors, fuel cells, water electrolysis. Thermofluids and thermal management |