Plegabilidad 90 ° en peso bruto: 2 - 5 [-]

Quick Comparison

Wrought Copper High Copper Alloy

ASTM B196 Grade C17200 TB00

Wrought Copper Nickel Silver Grade

UNS C77000 boway

Suministrada por:

Ningbo Boway Alloy Material

Wrought Copper Nickel Grade

UNS C70250 boway

Suministrada por:

Ningbo Boway Alloy Material

Bronce fosforado

UNS C52100 boway

Suministrada por:

Ningbo Boway Alloy Material

Bronce fosforado

UNS C51900 boway

Suministrada por:

Ningbo Boway Alloy Material

Bronce fosforado

UNS C52400 boway

Suministrada por:

Ningbo Boway Alloy Material

Wrought Copper High Copper Alloy

EN 1652 Grade C17200 TF00

Wrought Copper Nickel Grade

UNS C70318 boway

Suministrada por:

Ningbo Boway Alloy Material

Wrought Copper Nickel Grade

UNS C70250 boway

Suministrada por:

Ningbo Boway Alloy Material

Wrought Copper High Copper Alloy

STOL® 95 R540

Bronce fosforado

JIS C5240HQ Harada

Suministrada por:

HARADA METAL INDUSTRY CO., LTD.

Wrought Copper Nickel Grade

BrushForm® 158 Strip TM06 (C72900)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 158 Strip TM08 (C72900)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 96 TD04 Strip (C72700)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 96 TM06 Strip (C72700)

Suministrada por:

Materion Brush GmbH

Wrought Copper High Copper Alloy

Alloy 190 TM04 (C17200)

Suministrada por:

Materion Brush GmbH

Wrought Copper High Copper Alloy

Alloy 190 TM05 (C17200)

Suministrada por:

Materion Brush GmbH

Wrought Copper High Copper Alloy

Alloy 190 TM06 (C17200)

Suministrada por:

Materion Brush GmbH

Wrought Copper High Copper Alloy

Alloy 190 TM08 (C17200)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 96 TM08 Strip (C72700)

Suministrada por:

Materion Brush GmbH
Página 1 de 2