Malleable Cast Iron
SAE J158 Grade M3210 AnnealedMalleable Cast Iron
SAE J158 Grade M4504 Air quenched and TemperedMalleable Cast Iron
SAE J158 Grade M5003 Air quenched and TemperedMalleable Cast Iron
SAE J158 Grade M5503 Liquid quenched and TemperedMalleable Cast Iron
SAE J158 Grade M7002 Liquid quenched and TemperedMalleable Cast Iron
SAE J158 Grade M8501 Liquid quenched and TemperedPure/Low Nickel Alloy
DIN 17730 Grade G-Ni93C cast conditionAcero para herramientas y maquinaria
ISO 4957 Grade X210CrW12 quenched (+Q)Acero inoxidable austenítico
ASTM A312 Grade S31272White Cast Iron
EN 12513 Grade GJN-HV600(XCr14)White Cast Iron
EN 12513 Grade GJN-HV600(XCr18)White Cast Iron
EN 12513 Grade GJN-HV600(XCr23)Ductile (Nodular) Cast Iron
EN 12513 Grade GJN-HV600(XCr11)Acero para herramientas y maquinaria
ISO 4957 Grade X210Cr12 quenched (+Q)Hierro fundido
ASTM A571 Type D-2M Class 3 Heat-TreatedHierro fundido
ASTM A571 Type D-2M Class 4 Heat-TreatedHierro fundido
BS 4844 Grade 3D