ISO 4957 Grade X210CrW12 quenched (+Q)

Want to keep this datasheet? Save it now in your required format

Description

Properties: - high wear resistance and high a hardning ability with good dimensional stability - moderate toughness Application: - for high speedcut and stamping tool (also core lamination), roll and plate shear knifes for sheet thickness up to 2 mm - draw tools (die plates and mandrils), deep drawing tools, tools of the cold manufacturing of nuts and rivet - cold forging tools, flanges, bead and truing rolls - form and calibration rolls for the continuous profile and tubing production from strip steel of forming tools in ceramic industry and powder metallurgy - cut-off tools in the paper and plastic industry

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.76 g/cm³

Show Material materials with Density of 7.76 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

217.68 - 218 GPa

Show Material materials with Elastic modulus of 217.68 - 218 GPa

100.0 °C

213 GPa

Show Material materials with Elastic modulus of 213 GPa

200.0 °C

206 GPa

Show Material materials with Elastic modulus of 206 GPa

300.0 °C

198 GPa

Show Material materials with Elastic modulus of 198 GPa

400.0 °C

190 GPa

Show Material materials with Elastic modulus of 190 GPa

500.0 °C

180 GPa

Show Material materials with Elastic modulus of 180 GPa

600.0 °C

167 GPa

Show Material materials with Elastic modulus of 167 GPa

Poisson's ratio

20.0 °C

0.28 [-]

Show Material materials with Poisson's ratio of 0.28 [-]

Shear modulus

20.0 °C

84.95 GPa

Show Material materials with Shear modulus of 84.95 GPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

20.0 °C

1.02E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.02E-5 1/K

100.0 °C

1.05E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.05E-5 1/K

200.0 °C

1.09E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.09E-5 1/K

300.0 °C

1.13E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.13E-5 1/K

400.0 °C

1.16E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.16E-5 1/K

500.0 °C

1.2E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.2E-5 1/K

600.0 °C

1.22E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.22E-5 1/K

Unlock all property charts

Melting point

1370 - 1425 °C

Show Material materials with Melting point of 1370 - 1425 °C

Typical for Tool And Machining Steel

Specific heat capacity

20.0 °C

439 J/(kg·K)

Show Material materials with Specific heat capacity of 439 J/(kg·K)

100.0 °C

474 J/(kg·K)

Show Material materials with Specific heat capacity of 474 J/(kg·K)

200.0 °C

498 J/(kg·K)

Show Material materials with Specific heat capacity of 498 J/(kg·K)

300.0 °C

517 J/(kg·K)

Show Material materials with Specific heat capacity of 517 J/(kg·K)

400.0 °C

538 J/(kg·K)

Show Material materials with Specific heat capacity of 538 J/(kg·K)

500.0 °C

564 J/(kg·K)

Show Material materials with Specific heat capacity of 564 J/(kg·K)

600.0 °C

598 J/(kg·K)

Show Material materials with Specific heat capacity of 598 J/(kg·K)

Unlock all property charts

Thermal conductivity

20.0 °C

24 W/(m·K)

Show Material materials with Thermal conductivity of 24 W/(m·K)

100.0 °C

24.4 W/(m·K)

Show Material materials with Thermal conductivity of 24.4 W/(m·K)

200.0 °C

24.8 W/(m·K)

Show Material materials with Thermal conductivity of 24.8 W/(m·K)

300.0 °C

25.1 W/(m·K)

Show Material materials with Thermal conductivity of 25.1 W/(m·K)

400.0 °C

25.6 W/(m·K)

Show Material materials with Thermal conductivity of 25.6 W/(m·K)

500.0 °C

26.1 W/(m·K)

Show Material materials with Thermal conductivity of 26.1 W/(m·K)

600.0 °C

26.4 W/(m·K)

Show Material materials with Thermal conductivity of 26.4 W/(m·K)

Unlock all property charts

Thermal diffusivity

20.0 °C

7.1 mm²/s

Show Material materials with Thermal diffusivity of 7.1 mm²/s

100.0 °C

6.3 mm²/s

Show Material materials with Thermal diffusivity of 6.3 mm²/s

200.0 °C

6 mm²/s

Show Material materials with Thermal diffusivity of 6 mm²/s

300.0 °C

5.7 mm²/s

Show Material materials with Thermal diffusivity of 5.7 mm²/s

400.0 °C

5.4 mm²/s

Show Material materials with Thermal diffusivity of 5.4 mm²/s

500.0 °C

4.9 mm²/s

Show Material materials with Thermal diffusivity of 4.9 mm²/s

600.0 °C

4.1 mm²/s

Show Material materials with Thermal diffusivity of 4.1 mm²/s

Unlock all property charts

Electrical

PropertyTemperatureValue

Electrical resistivity

20.0 °C

6.03E-7 Ω·m

Show Material materials with Electrical resistivity of 6.03E-7 Ω·m

100.0 °C

6.68E-7 Ω·m

Show Material materials with Electrical resistivity of 6.68E-7 Ω·m

200.0 °C

7.43E-7 Ω·m

Show Material materials with Electrical resistivity of 7.43E-7 Ω·m

300.0 °C

8.17E-7 Ω·m

Show Material materials with Electrical resistivity of 8.17E-7 Ω·m

400.0 °C

8.9E-7 Ω·m

Show Material materials with Electrical resistivity of 8.9E-7 Ω·m

500.0 °C

9.62E-7 Ω·m

Show Material materials with Electrical resistivity of 9.62E-7 Ω·m

600.0 °C

1.04E-6 Ω·m

Show Material materials with Electrical resistivity of 1.04E-6 Ω·m

Unlock all property charts

Chemical properties

PropertyValue

Carbon

2 - 2.25 %

Show Material materials with Carbon of 2 - 2.25 %

Chromium

11 - 12 %

Show Material materials with Chromium of 11 - 12 %

Manganese

0.15 - 0.45 %

Show Material materials with Manganese of 0.15 - 0.45 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

0.1 - 0.4 %

Show Material materials with Silicon of 0.1 - 0.4 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %

Tungsten

0.6 - 0.8 %

Show Material materials with Tungsten of 0.6 - 0.8 %