ASTM B534 Grade C17500 TD04

Want to keep this datasheet? Save it now in your required format

Description

Alloy 10 from Materion Performance Alloys provides high electrical and thermal conductivity coupled with moderate strength.

Related Standards

Equivalent Materials

This material data has been provided by MakeItFrom.com,Materion Brush GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.83 - 8.9 g/cm³

Show Material materials with Density of 8.83 - 8.9 g/cm³

Dimension

PropertyValueComment

Diameter

1.27 - 12.7 mm

Show Material materials with Diameter of 1.27 - 12.7 mm

Length

610 - 91000 mm

Show Material materials with Length of 610 - 91000 mm

max. Rod and Bar

Outside diameter

0.76 - 76 mm

Show Material materials with Outside diameter of 0.76 - 76 mm

Rod

Thickness

0.76 - 76 mm

Show Material materials with Thickness of 0.76 - 76 mm

Bar

Width

305 - 559 mm

Show Material materials with Width of 305 - 559 mm

Wall thickness

Typically 10 to 20% of OD

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

138 - 140 GPa

Show Material materials with Elastic modulus of 138 - 140 GPa

Elongation

23.0 °C

2 - 20 %

Show Material materials with Elongation of 2 - 20 %

Tensile strength

23.0 °C

440 - 590 MPa

Show Material materials with Tensile strength of 440 - 590 MPa

Yield strength

23.0 °C

470 MPa

Show Material materials with Yield strength of 470 MPa

Yield strength Rp0.2

23.0 °C

340 - 550 MPa

Show Material materials with Yield strength Rp0.2 of 340 - 550 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.76E-5 - 1.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.76E-5 - 1.8E-5 1/K

Melting point

1010 - 1020 °C

Show Material materials with Melting point of 1010 - 1020 °C

Specific heat capacity

23.0 °C

340 J/(kg·K)

Show Material materials with Specific heat capacity of 340 J/(kg·K)

Thermal conductivity

23.0 °C

200 W/(m·K)

Show Material materials with Thermal conductivity of 200 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

2.9E-6 - 3.8E-6 Ω·m

Show Material materials with Electrical resistivity of 2.9E-6 - 3.8E-6 Ω·m

Specific Electrical conductivity

45 - 60 % IACS

Show Material materials with Specific Electrical conductivity of 45 - 60 % IACS

Chemical properties

PropertyValueComment

Aluminium

0 - 0.2 %

Show Material materials with Aluminium of 0 - 0.2 %

Beryllium

0.4 - 0.7 %

Show Material materials with Beryllium of 0.4 - 0.7 %

Cobalt

2.4 - 2.7 %

Show Material materials with Cobalt of 2.4 - 2.7 %

Copper

95.6 - 97.2 %

Show Material materials with Copper of 95.6 - 97.2 %

Balance

Iron

0 - 0.1 %

Show Material materials with Iron of 0 - 0.1 %

Other

0 - 0.5 %

Show Material materials with Other of 0 - 0.5 %

Silicon

0 - 0.2 %

Show Material materials with Silicon of 0 - 0.2 %

Technological properties

Property
Application areas

Typical applications include resistance welding components, and inserts for metal die casting, injection molding and blow molding.,Typical applications include dies casting plunger tips and dies for steel extrusion.,Typical applications include heat exchanger tubing and resistance welding components.,Typical applications include coil springs and formed wire contacts.