Nickel Molybdenum Steel
ASTM A387 Grade 11 Class 1, Annealed, Normalized and Tempered, or Quenched and TemperedSuministrada por:
1 proveedor Matmatch
Acero inoxidable ferrítico
DIN 17440 Grade X6Cr17 soft annealed (+A)Acero inoxidable ferrítico
DIN 17440 Grade X3CrTi17 soft annealed (+A)Acero inoxidable ferrítico
EN 10088-1 Grade X3CrNb17 soft annealed (+A)Aleación alfa-beta
DIN 17851 Grade TiAl6V6Sn2 AnnealedPoliéter éter cetona (PEEK)
Polyetheretherketone Reinforced with 30% Carbon Fibre (PEEK+CF30)Suministrada por:
2 proveedores de Matmatch
Acero inoxidable ferrítico
EN 10088-1 Grade X6CrMo17-1 soft annealed (+A)Acero inoxidable ferrítico
EN 10088-1 Grade X3CrTi17 soft annealed (+A)Aleación casi alfa
VdTÜV WB 230-3 Grade TiNi0.8Mo0.3 AnnealedSuministrada por:
2 proveedores de Matmatch