Polyetheretherketone Reinforced with 30% Carbon Fibre (PEEK+CF30)

Alternative and trade names
Victrex™, Vestakeep®, KetaSpire®, TECACOMP®
Want to keep this datasheet? Save it now in your required format

Description

30% carbon-fiber reinforced grade of polyetheretherketone (PEEK, engineering plastic). Carbon- fiber reinforcement of PEEK provides the maximum levels of mechanical properties at temperatures approaching 300°C, and the lowest coefficient of linear thermal expansion.


It is produced to the highest industry standards and is characterized by a distinct combination of properties, which include excellent wear resistance, best-in-class fatigue resistance, ease of melt processing, high purity, and excellent chemical resistance to organics, acids and bases.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.4 - 1.44 g/cm³

Show Material materials with Density of 1.4 - 1.44 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

22.0 - 28.0 GPa

Show Material materials with Elastic modulus of 22.0 - 28.0 GPa

Elongation

1.5 - 2.0 %

Show Material materials with Elongation of 1.5 - 2.0 %

Impact strength, Charpy notched

6.0 - 10.0 kJ/m²

Show Material materials with Impact strength, Charpy notched of 6.0 - 10.0 kJ/m²

Impact strength, Charpy unnotched

33 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 33 kJ/m²

60 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 60 kJ/m²

Tensile strength

220.0 - 275.0 MPa

Show Material materials with Tensile strength of 220.0 - 275.0 MPa

at 1.5-2% strain

Thermal

PropertyValue

Coefficient of thermal expansion

4e-06 - 3.8e-05 1/K

Show Material materials with Coefficient of thermal expansion of 4e-06 - 3.8e-05 1/K

Melting point

340.0 - 343.0 °C

Show Material materials with Melting point of 340.0 - 343.0 °C

Specific heat capacity

1800.0 - 1850.0 J/(kg·K)

Show Material materials with Specific heat capacity of 1800.0 - 1850.0 J/(kg·K)

Thermal conductivity

0.92 - 0.95 W/(m·K)

Show Material materials with Thermal conductivity of 0.92 - 0.95 W/(m·K)

Flammability

UL 94 V0

Electrical

PropertyValue

Dielectric constant

17 [-]

Show Material materials with Dielectric constant of 17 [-]

Electrical resistivity

1000000.0 - 1000000000000.0 Ω·m

Show Material materials with Electrical resistivity of 1000000.0 - 1000000000000.0 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

oil scavenger lines, rod benders, medical devices, pump parts, surgical instruments

Fillers

30% Carbon Fiber

Other

You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application:

Polymer Advanced Search

Processing methods

Injection molding, extrusion