General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.36 g/cm³ Show Supplier Material materials with Density of 1.36 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.6 % Show Supplier Material materials with Moisture absorption of 1.6 % | dry | Sim. to ISO 62 |
Water absorption | 6 % Show Supplier Material materials with Water absorption of 6 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | -40 °C | 10.5 GPa Show Supplier Material materials with Elastic modulus of 10.5 GPa | dry | ISO 527-1/-2 |
7.5 GPa Show Supplier Material materials with Elastic modulus of 7.5 GPa | conditioned | ISO 527-1/-2 | ||
10 GPa Show Supplier Material materials with Elastic modulus of 10 GPa | dry | ISO 527-1/-2 | ||
100 °C | 4.8 GPa Show Supplier Material materials with Elastic modulus of 4.8 GPa | dry | ISO 527-1/-2 | |
Elongation | -40 °C | 3.4 % Show Supplier Material materials with Elongation of 3.4 % | dry | ISO 527-1/-2 |
3.6 % Show Supplier Material materials with Elongation of 3.6 % | dry | ISO 527-1/-2 | ||
5 % Show Supplier Material materials with Elongation of 5 % | conditioned | ISO 527-1/-2 | ||
Flexural modulus | 6.4 GPa Show Supplier Material materials with Flexural modulus of 6.4 GPa | conditioned | ISO 178 | |
9.3 GPa Show Supplier Material materials with Flexural modulus of 9.3 GPa | dry | ISO 178 | ||
Flexural yield strength | 200 MPa Show Supplier Material materials with Flexural yield strength of 200 MPa | conditioned | ISO 178 | |
295 MPa Show Supplier Material materials with Flexural yield strength of 295 MPa | dry | ISO 178 | ||
Impact strength, Charpy notched | -30 °C | 10 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 10 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 12 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 12 kJ/m² | dry | ISO 179/1eA | |
23 °C | 20 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 20 kJ/m² | conditioned | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 70 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 70 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 80 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 80 kJ/m² | dry | ISO 179/1eU | |
23 °C | 100 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 100 kJ/m² | conditioned | ISO 179/1eU | |
Tensile strength | -40 °C | 255 MPa Show Supplier Material materials with Tensile strength of 255 MPa | dry | ISO 527-1/-2 |
140 MPa Show Supplier Material materials with Tensile strength of 140 MPa | conditioned | ISO 527-1/-2 | ||
205 MPa Show Supplier Material materials with Tensile strength of 205 MPa | dry | ISO 527-1/-2 | ||
100 °C | 110 MPa Show Supplier Material materials with Tensile strength of 110 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 2e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
7e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 7e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Flammability | HB | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Heat deflection temperature | 245 °C Show Supplier Material materials with Heat deflection temperature of 245 °C | dry | ISO 75-1/-2 | 2 MPa | ||
260 °C Show Supplier Material materials with Heat deflection temperature of 260 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Melting point | 260 °C Show Supplier Material materials with Melting point of 260 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 0.71 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 0.71 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 0.71 mm |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | dry, conditioned | IEC 60112 | |
Dielectric constant | 3.5 [-] Show Supplier Material materials with Dielectric constant of 3.5 [-] | dry | IEC 62631-2-1 | 1MHz |
3.8 [-] Show Supplier Material materials with Dielectric constant of 3.8 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.6 [-] Show Supplier Material materials with Dielectric constant of 4.6 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
11 [-] Show Supplier Material materials with Dielectric constant of 11 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Dielectric strength | 25 kV/mm Show Supplier Material materials with Dielectric strength of 25 kV/mm | conditioned | IEC 60243-1 | |
30 kV/mm Show Supplier Material materials with Dielectric strength of 30 kV/mm | dry | IEC 60243-1 | ||
Dissipation factor | 90 [-] Show Supplier Material materials with Dissipation factor of 90 [-] | dry | IEC 62631-2-1 | 100Hz |
160 [-] Show Supplier Material materials with Dissipation factor of 160 [-] | dry | IEC 62631-2-1 | 1MHz | |
1000 [-] Show Supplier Material materials with Dissipation factor of 1000 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
1400 [-] Show Supplier Material materials with Dissipation factor of 1400 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Shrinkage | 0.2 % Show Supplier Material materials with Shrinkage of 0.2 % | dry | Sim. to ISO 294-4 | Parallel |
1.2 % Show Supplier Material materials with Shrinkage of 1.2 % | dry | Sim. to ISO 294-4 | Normal | |
Specific heat capacity melt | 2170 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2170 J/(kg·K) | dry | - | |
Thermal conductivity of melt | 0.172 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.172 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 30% Glass Fiber |