Akulon® S223-G6-FC BK00001

Alternative and trade names
PA66-GF30
Want to keep this datasheet? Save it now in your required format

Description

Akulon® is our family of high performance polyamide 6 and polyamide 66 materials, used by customers across the world in applications ranging from automotive, electronics & electrical, to furniture and packaging.
We offer Akulon® grades for injection molding, blow molding and extrusion (including barrier film, stock shapes, convoluted tubes, and mono and multi filament).
In molded parts the material offers an excellent balance of easy design and processing with outstanding mechanical properties over a wide temperature range and in diverse conditions. Meanwhile for extrusion the strength, resilience and easy processing of Akulon® sets the market standards.

Datasheet URL:

Akulon® S223-G6-FC BK00001

This material data has been provided by DSM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Density

1.36 g/cm³

Show Supplier Material materials with Density of 1.36 g/cm³

dry

ISO 1183

Moisture absorption

1.6 %

Show Supplier Material materials with Moisture absorption of 1.6 %

dry

Sim. to ISO 62

Water absorption

6 %

Show Supplier Material materials with Water absorption of 6 %

dry

Sim. to ISO 62

Mechanical

PropertyTemperatureValueConditionTesting Standard

Elastic modulus

7.5 GPa

Show Supplier Material materials with Elastic modulus of 7.5 GPa

conditioned

ISO 527-1/-2

9.5 GPa

Show Supplier Material materials with Elastic modulus of 9.5 GPa

dry

ISO 527-1/-2

Elongation

3 %

Show Supplier Material materials with Elongation of 3 %

dry

ISO 527-1/-2

5 %

Show Supplier Material materials with Elongation of 5 %

conditioned

ISO 527-1/-2

Flexural modulus

8.4 GPa

Show Supplier Material materials with Flexural modulus of 8.4 GPa

dry

ISO 178

Flexural yield strength

250 MPa

Show Supplier Material materials with Flexural yield strength of 250 MPa

dry

ISO 178

Impact strength, Charpy notched

-30 °C

10 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 10 kJ/m²

dry, conditioned

ISO 179/1eA

23 °C

12 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 12 kJ/m²

dry

ISO 179/1eA

23 °C

20 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 20 kJ/m²

conditioned

ISO 179/1eA

Impact strength, Charpy unnotched

-30 °C

70 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 70 kJ/m²

dry, conditioned

ISO 179/1eU

23 °C

80 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 80 kJ/m²

dry

ISO 179/1eU

23 °C

100 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 100 kJ/m²

conditioned

ISO 179/1eU

Tensile strength

140 MPa

Show Supplier Material materials with Tensile strength of 140 MPa

conditioned

ISO 527-1/-2

190 MPa

Show Supplier Material materials with Tensile strength of 190 MPa

dry

ISO 527-1/-2

Thermal

PropertyValueConditionTesting StandardPressureThicknessComment

Coefficient of thermal expansion

2e-07 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 2e-07 1/K

dry

ISO 11359-1/-2

Parallel

7e-07 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 7e-07 1/K

dry

ISO 11359-1/-2

Normal

Heat deflection temperature

245 °C

Show Supplier Material materials with Heat deflection temperature of 245 °C

dry

ISO 75-1/-2

2 MPa

260 °C

Show Supplier Material materials with Heat deflection temperature of 260 °C

dry

ISO 75-1/-2

0.45 MPa

Melting point

260 °C

Show Supplier Material materials with Melting point of 260 °C

dry

ISO 11357-1/-3

10°C/min

Relative temperature index, electrical

65 °C

Show Supplier Material materials with Relative temperature index, electrical of 65 °C

dry

UL746B

0.71 mm

Relative temperature index, mechanical impact

65 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C

dry

UL746B

0.71 mm

Relative temperature index, mechanical strength

65 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C

dry

UL746B

0.71 mm

Electrical

PropertyValueConditionTesting StandardComment

Comparative tracking index

600 V

Show Supplier Material materials with Comparative tracking index of 600 V

dry, conditioned

IEC 60112

Dielectric constant

3.5 [-]

Show Supplier Material materials with Dielectric constant of 3.5 [-]

dry

IEC 62631-2-1

1MHz

3.8 [-]

Show Supplier Material materials with Dielectric constant of 3.8 [-]

dry

IEC 62631-2-1

100Hz

4.6 [-]

Show Supplier Material materials with Dielectric constant of 4.6 [-]

conditioned

IEC 62631-2-1

1MHz

11 [-]

Show Supplier Material materials with Dielectric constant of 11 [-]

conditioned

IEC 62631-2-1

100Hz

Dielectric strength

25 kV/mm

Show Supplier Material materials with Dielectric strength of 25 kV/mm

conditioned

IEC 60243-1

30 kV/mm

Show Supplier Material materials with Dielectric strength of 30 kV/mm

dry

IEC 60243-1

Dissipation factor

90 [-]

Show Supplier Material materials with Dissipation factor of 90 [-]

dry

IEC 62631-2-1

100Hz

160 [-]

Show Supplier Material materials with Dissipation factor of 160 [-]

dry

IEC 62631-2-1

1MHz

1000 [-]

Show Supplier Material materials with Dissipation factor of 1000 [-]

conditioned

IEC 62631-2-1

1MHz

1400 [-]

Show Supplier Material materials with Dissipation factor of 1400 [-]

conditioned

IEC 62631-2-1

100Hz

Surface resistivity

1e+14 Ω/sq

Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq

conditioned

IEC 62631-3-2

Volume resistivity

1e+11 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm

conditioned

IEC 62631-3-1

1e+13 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm

dry

IEC 62631-3-1

Rheological Properties

PropertyValueConditionTesting StandardComment

Shrinkage

0.2 %

Show Supplier Material materials with Shrinkage of 0.2 %

dry

Sim. to ISO 294-4

Parallel

1.2 %

Show Supplier Material materials with Shrinkage of 1.2 %

dry

Sim. to ISO 294-4

Normal

Specific heat capacity melt

2170 J/(kg·K)

Show Supplier Material materials with Specific heat capacity melt of 2170 J/(kg·K)

dry

-

Thermal conductivity of melt

0.172 W/(m·K)

Show Supplier Material materials with Thermal conductivity of melt of 0.172 W/(m·K)

dry

-

Technological properties

Property
Application areas

Spatulas and Kitchenware

Certifications

Food Contact

Fillers

30% Glass Fiber