Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMo4-5 normalized and tempered (+NT)Suministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMo4-5 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Wrought Copper High Copper Alloy
ASTM B194 Grade C17200 TD04Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TH04Wrought Copper High Copper Alloy
EN 1652 Grade C17200 TF00Chromium Molybdenum Steel
EN 10216-2 Grade 13CrMo4-5 normalized and tempered (+NT)Silicon Steel
EN 10089 Grade 38Si7 quenched and tempered (+QT)Chromium Molybdenum Steel
EN 10222-2 Grade 13CrMo4-5 normalized and tempered (+NT)Chromium Molybdenum Steel
EN 10222-2 Grade 13CrMo4-5 quenched and tempered (+QT)Chromium Molybdenum Steel
EN 10273 Grade 13CrMo4-5 normalized and tempered (+NT)Chromium Molybdenum Steel
DIN 17155 Grade 13CrMo4-4 quenched and tempered (+QT)Silicon Steel
DIN 17222 Grade 71Si7 cold rolled and hardenedChromium Molybdenum Steel
EN 10273 Grade 13CrMo4-5 normalized and tempered or quenched and temperedChromium Molybdenum Steel
EN 10273 Grade 13CrMo4-5 quenched and tempered (+QT)Silicon Manganese Steel
EN 10132-4 Grade 71Si7 cold rolled, quenched and tempered (+C+QT)Acero para herramientas y maquinaria
ISO 4957 Grade 60MnSiCr4