Acero inoxidable austenítico
Alloy 24 / 1.4565 Solution annealed and quenchedSuministrada por:
Hempel Special MetalsAcero inoxidable austenítico
EN 10088-1 Grade X2CrNiMoN17-13-5 solution annealed (+AT)Acero inoxidable austenítico
EN 10088-1 Grade X1CrNiMoN25-22-2 solution annealed (+AT)Acero inoxidable austenítico
EN 10088-1 Grade X2CrNiMoN17-13-3 solution annealed (+AT)