Módulo de flexión: 1.74 GPa

Quick Comparison

Polyvinylidenefluoride (PVDF)

Kynar® 720

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 720 RED

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 740

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 740 RED

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 720 MED

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 710

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 9000 HD

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 460

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 761

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 705

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 760

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 761A

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 1000 HD

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 741

Suministrada por:

Arkema: High Performance Polymers

Mezcla de polímeros

FLEX NORYL™ Resin WCV072 - Americas

Suministrada por:

Sabic

Mezcla de polímeros

FLEX NORYL™ Resin WCV072 - Europe

Suministrada por:

Sabic

Mezcla de polímeros

FLEX NORYL™ Resin WCV072 - Asia

Suministrada por:

Sabic

Thermoplastic Polyolefin (TPO)

SABIC® PPcompound 8620

Polyvinylidenefluoride (PVDF)

Kynar® HSV 900

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® MG15

Suministrada por:

Arkema: High Performance Polymers
Página 1 de 2