Kynar® 1000 HD

Alternative and trade names
PVDF
Want to keep this datasheet? Save it now in your required format

Description

Kynar® resins are fluorinated thermoplastic homopolymers.

Outstanding characteristics: chemical resistance, imperviousness to UV, high barrier properties, high purity, good mechanical and thermo mechanical properties.

Kynar® 1000 HD resin is a standard grade of granules for compression and transfer molding, for extrusion of thick walled parts: blocks, rods, plaques, tubes.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.77 g/cm³

Show Supplier Material materials with Density of 1.77 g/cm³

ISO 1183

Limiting oxygen index

23.0 °C

83 %

Show Supplier Material materials with Limiting oxygen index of 83 %

ISO 4589-1/-2

Moisture absorption

23.0 °C

0.02 %

Show Supplier Material materials with Moisture absorption of 0.02 %

Sim. to ISO 62

Water absorption

23.0 °C

0.03 %

Show Supplier Material materials with Water absorption of 0.03 %

Sim. to ISO 62

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2 GPa

Show Supplier Material materials with Elastic modulus of 2 GPa

ISO 527-1/-2

Elongation

23.0 °C

50 %

Show Supplier Material materials with Elongation of 50 %

min., ISO 527-1/-2, nominal

Elongation at yield

23.0 °C

9 %

Show Supplier Material materials with Elongation at yield of 9 %

ISO 527-1/-2

Impact strength, Charpy notched

-30.0 °C

5 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 5 kJ/m²

ISO 179/1eA

23.0 °C

22 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 22 kJ/m²

ISO 179/1eA

Yield strength

23.0 °C

50 MPa

Show Supplier Material materials with Yield strength of 50 MPa

ISO 527-1/-2

Impact strength, Charpy unnotched

No break @ 23,-30°C, ISO 179/1eU

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.5E-4 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.5E-4 1/K

ISO 11359-1/-2

Glass transition temperature

-40 °C

Show Supplier Material materials with Glass transition temperature of -40 °C

ISO 11357-1/-2, 10°C/min

Heat deflection temperature, 1.80 MPa

104 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 104 °C

ISO 75-1/-2

Melting point

169 °C

Show Supplier Material materials with Melting point of 169 °C

ISO 11357-1/-3, 10°C/min

Relative temperature index, electrical

150 °C

Show Supplier Material materials with Relative temperature index, electrical of 150 °C

UL 746B

Relative temperature index, mechanical strength

150 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 150 °C

UL 746B

Specific heat capacity

23.0 °C

745 - 958 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 745 - 958 J/(kg·K)

DSC

Thermal decomposition in air

375 °C

Show Supplier Material materials with Thermal decomposition in air of 375 °C

TGA, 1% wt. loss

Thermal decomposition in nitrogen

410 °C

Show Supplier Material materials with Thermal decomposition in nitrogen of 410 °C

TGA, 1% wt. loss

Vicat softening temperature

138 °C

Show Supplier Material materials with Vicat softening temperature of 138 °C

ISO 306, 50°C/h 50N

Flammability

At thickness 1.6 mm IEC 60695-11-10: V-0, At thickness 0.8 mm IEC 60695-11-10: V-0

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

600 V

Show Supplier Material materials with Comparative tracking index of 600 V

IEC 60112

Dielectric constant, 100Hz

23.0 °C

10.5 [-]

Show Supplier Material materials with Dielectric constant, 100Hz of 10.5 [-]

IEC 60250

Dielectric constant, 1MHz

23.0 °C

7 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 7 [-]

IEC 60250

Dielectric strength

23.0 °C

27 kV/mm

Show Supplier Material materials with Dielectric strength of 27 kV/mm

IEC 60243-1

Dissipation factor, 100Hz

23.0 °C

0.03 [-]

Show Supplier Material materials with Dissipation factor, 100Hz of 0.03 [-]

IEC 60250

Dissipation factor, 1MHz

23.0 °C

0.24 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 0.24 [-]

IEC 60250

Volume resistivity

23.0 °C

2.30E+12 Ω·cm

Show Supplier Material materials with Volume resistivity of 2.30E+12 Ω·cm

IEC 60093

Rheological Properties

PropertyTemperatureValueComment

Melt volume-flow rate

1.1 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 1.1 cm³/10min

ISO 1133, 230°C/5kg

Shrinkage

23.0 °C

2 %

Show Supplier Material materials with Shrinkage of 2 %

ISO 294-4 2577

Shrinkage, transverse

23.0 °C

2 %

Show Supplier Material materials with Shrinkage, transverse of 2 %

ISO 294-4 2577

Technological properties

Property
Application areas

Main applications:

  • corrosion protection in the chemical industry
  • coating (painting, co-extrusion)
  • off shore
  • wire and cable

    or

    Chemical Process Industry,Chemical Process Industry - High Purity Piping,Chemical Process Industry - Injection Molding,Chemical Process Industry - Stock Shapes,Plenum Pipe,Tubing and Hoses