Kynar® HSV 900

Alternative and trade names
PVDF
Want to keep this datasheet? Save it now in your required format

Description

Kynar® resins are fluorinated thermoplastic homopolymers. Outstanding characteristics: chemical resistance, imperviousness to UV, high barrier properties, high purity, good mechanical and thermo-mechanical properties.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.77 - 1.79 g/cm³

Show Supplier Material materials with Density of 1.77 - 1.79 g/cm³

ASTM D792

Limiting oxygen index

23.0 °C

44 %

Show Supplier Material materials with Limiting oxygen index of 44 %

ASTM D2863

Mechanical

PropertyTemperatureValueComment

Compressive strength

23.0 °C

68.9 - 103 MPa

Show Supplier Material materials with Compressive strength of 68.9 - 103 MPa

ASTM D695

Elongation

23.0 °C

50 - 250 %

Show Supplier Material materials with Elongation of 50 - 250 %

ASTM D638

Flexural modulus

23.0 °C

1.38 - 2.21 GPa

Show Supplier Material materials with Flexural modulus of 1.38 - 2.21 GPa

ASTM D790

Hardness, Shore D

23.0 °C

76 - 80 [-]

Show Supplier Material materials with Hardness, Shore D of 76 - 80 [-]

ASTM D2240

Impact strength, Charpy notched, ASTM

23.0 °C

107 - 320 J/m

Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 107 - 320 J/m

ASTM D256

Tensile strength

23.0 °C

34 - 43 MPa

Show Supplier Material materials with Tensile strength of 34 - 43 MPa

ASTM D638

Yield strength

23.0 °C

40 - 55.2 MPa

Show Supplier Material materials with Yield strength of 40 - 55.2 MPa

ASTM D638

Thermal

PropertyValueComment

Melting point

165 - 342 °C

Show Supplier Material materials with Melting point of 165 - 342 °C

ASTM D3418

Optical

PropertyValueComment

Refractive index

1.42 [-]

Show Supplier Material materials with Refractive index of 1.42 [-]

ASTM D542, sodium D line

Rheological Properties

PropertyTemperatureValueComment

Melt viscosity

23.0 °C

7000 - 7500 Pa·s

Show Supplier Material materials with Melt viscosity of 7000 - 7500 Pa·s

ASTM D3835

Technological properties

Property
Application areas

Lithium Ion Battery Binder