RADISTRONG A RV500UK 3010 BK

Alternative and trade names
PA66-GF50
Want to keep this datasheet? Save it now in your required format

Description

Special PA 50% glass fibre reinforced, injection moulding grade. Improved UV resistance. Black colour

Product with enhanced mechanical properties, suitable for demanding applications as in case of metal replacement. Intended to resist to outdoor exposure

This material data has been provided by Radici Group.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting StandardThickness

Density

1.6 g/cm³

Show Supplier Material materials with Density of 1.6 g/cm³

dry

ISO 1183

Moisture absorption

0.9 %

Show Supplier Material materials with Moisture absorption of 0.9 %

50% RH

ISO 62

2 mm

Water absorption

3.8 %

Show Supplier Material materials with Water absorption of 3.8 %

ISO 62

2 mm

Mechanical

PropertyTemperatureValueConditionTesting StandardComment

Elastic modulus

18 GPa

Show Supplier Material materials with Elastic modulus of 18 GPa

dry

ISO 527-2/1A

1mm/min

Elongation

2 %

Show Supplier Material materials with Elongation of 2 %

dry

ISO 527-2/1A

5mm/min

Flexural modulus

16 GPa

Show Supplier Material materials with Flexural modulus of 16 GPa

dry

ISO 178

2mm/min

Flexural strength

360 MPa

Show Supplier Material materials with Flexural strength of 360 MPa

dry

ISO 178

2mm/min

Impact strength, Charpy notched

-30 °C

13 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 13 kJ/m²

dry

ISO 179/1eA

23 °C

13 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 13 kJ/m²

dry

ISO 179/1eA

Impact strength, Charpy unnotched

-30 °C

75 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 75 kJ/m²

dry

ISO 179/1eU

23 °C

90 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 90 kJ/m²

dry

ISO 179/1eU

Unlock all property charts

Tensile strength

250 MPa

Show Supplier Material materials with Tensile strength of 250 MPa

dry

ISO 527-2/1A

5mm/min

Thermal

PropertyValueThicknessTesting StandardPressureComment

Glow Wire Flammability Index

650 °C

Show Supplier Material materials with Glow Wire Flammability Index of 650 °C

1 mm, 2 mm

IEC 60695-2-12

Heat deflection temperature

245 °C

Show Supplier Material materials with Heat deflection temperature of 245 °C

ISO 75/2Af

2 MPa

Melting point

258 °C

Show Supplier Material materials with Melting point of 258 °C

ISO 11357-1/-3

10°C/min

Flammability

Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3

Electrical

PropertyValueConditionTesting StandardComment

Surface resistivity

1e+10 Ω/sq

Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq

50%RH

IEC 60093

500V

1e+12 Ω/sq

Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq

dry

IEC 60093

500V

Volume resistivity

1e+12 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm

50%RH

IEC 60093

500V

1e+14 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+14 Ω·cm

dry

IEC 60093

500V

Rheological Properties

PropertyValueConditionTesting StandardComment

Shrinkage

0.1 %

Show Supplier Material materials with Shrinkage of 0.1 %

dry

ISO 294-4

0.4 %

Show Supplier Material materials with Shrinkage of 0.4 %

dry

ISO 294-4

Transverse

Technological properties

Property
Certifications

RoHS 2011/65/UE

Color

Black

Fillers

50% Glass Fiber

Processing methods

Injection Molding