Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Wrought Copper High Copper Alloy
EN 1652 Grade C17200 TF00Wrought Copper Nickel Grade
HARDIALL® - TS 160 U - CuNi15Sn8 - C72900Suministrada por:
Lebronze AlloysWrought Copper High Copper Alloy
EN 1652 Grade CuBe2 TH