Heat deflection temperature, 1.80 MPa: 218 °C

Quick Comparison

Poliéter éter cetona (PEEK)

TECACOMP PEEK LDS black 1047045

Suministrada por:

Ensinger GmbH

Polietileno tereftalato (PET)

Rynite® FR531 NC010

Polyamide 6 (PA6)

Zytel® 73G45 BK263

Polieterimida (PEI)

ULTEM™ Resin CRS5211R - Americas

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin CRS5211R - Asia

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ STAT-KON™ Compound RX04031

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin CRS5311 - Americas

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin CRS5311 - Asia

Suministrada por:

Sabic

Polietersulfona (PES)

LNP™ THERMOCOMP™ Compound JX97000

Suministrada por:

Sabic

Polietersulfona (PES)

LNP™ THERMOCOMP™ Compound JF004E - Asia

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin CRS5201R - Americas

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin CRS5201R - Asia

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin CRS5201 - Asia

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin CRS5201 - Americas

Suministrada por:

Sabic

Polietersulfona (PES)

LNP™ THERMOCOMP™ Compound JF004 - Asia

Suministrada por:

Sabic