General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.27 g/cm³ Show Supplier Material materials with Density of 1.27 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.6 % Show Supplier Material materials with Moisture absorption of 2.6 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 3.6 GPa Show Supplier Material materials with Elastic modulus of 3.6 GPa | conditioned | ISO 527-1/-2 | |
7.0 GPa Show Supplier Material materials with Elastic modulus of 7.0 GPa | dry | ISO 527-1/-2 | ||
120 °C | 2.4 GPa Show Supplier Material materials with Elastic modulus of 2.4 GPa | dry | ISO 527-1/-2 | |
160 °C | 2.1 GPa Show Supplier Material materials with Elastic modulus of 2.1 GPa | dry | ISO 527-1/-2 | |
200 °C | 1.6 GPa Show Supplier Material materials with Elastic modulus of 1.6 GPa | dry | ISO 527-1/-2 | |
Elongation | 3.5 % Show Supplier Material materials with Elongation of 3.5 % | dry | ISO 527-1/-2 | |
20 % Show Supplier Material materials with Elongation of 20 % | conditioned | ISO 527-1/-2 | ||
120 °C | 12 % Show Supplier Material materials with Elongation of 12 % | dry | ISO 527-1/-2 | |
160 °C | 12 % Show Supplier Material materials with Elongation of 12 % | dry | ISO 527-1/-2 | |
200 °C | 13 % Show Supplier Material materials with Elongation of 13 % | dry | ISO 527-1/-2 | |
Flexural modulus | 2.8 GPa Show Supplier Material materials with Flexural modulus of 2.8 GPa | conditioned | ISO 178 | |
5.7 GPa Show Supplier Material materials with Flexural modulus of 5.7 GPa | dry | ISO 178 | ||
Flexural yield strength | 85 MPa Show Supplier Material materials with Flexural yield strength of 85 MPa | conditioned | ISO 178 | |
195 MPa Show Supplier Material materials with Flexural yield strength of 195 MPa | dry | ISO 178 | ||
Impact strength, Charpy notched | -30 °C | 3 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 3 kJ/m² | conditioned | ISO 179/1eA |
-30 °C | 6 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 6 kJ/m² | dry | ISO 179/1eA | |
23 °C | 12 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 12 kJ/m² | dry | ISO 179/1eA | |
23 °C | 14.0 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 14.0 kJ/m² | conditioned | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 41 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 41 kJ/m² | conditioned | ISO 179/1eU |
-30 °C | 63 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 63 kJ/m² | dry | ISO 179/1eU | |
23 °C | 74 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 74 kJ/m² | dry | ISO 179/1eU | |
23 °C | 95 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 95 kJ/m² | conditioned | ISO 179/1eU | |
Tensile strength | 57.0 MPa Show Supplier Material materials with Tensile strength of 57.0 MPa | conditioned | ISO 527-1/-2 | |
135 MPa Show Supplier Material materials with Tensile strength of 135 MPa | dry | ISO 527-1/-2 | ||
120 °C | 60 MPa Show Supplier Material materials with Tensile strength of 60 MPa | dry | ISO 527-1/-2 | |
160 °C | 50 MPa Show Supplier Material materials with Tensile strength of 50 MPa | dry | ISO 527-1/-2 | |
200 °C | 37 MPa Show Supplier Material materials with Tensile strength of 37 MPa | dry | ISO 527-1/-2 |
Thermal
Technological properties
Property | ||
---|---|---|
Fillers | 20% Glass Fiber |