Resistencia al choque, ensayo Charpy no entallado: 96 kJ/m²

Quick Comparison

Polyamide 11 (PA11)

Rilsan® BZM 30 O TL

Suministrada por:

Arkema: High Performance Polymers

Polyamide 6 (PA6)

Novamid® 1015GH35 BK37

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Novamid® 1015G35 NAT

Suministrada por:

DSM Engineering Materials

Polyamide 11 (PA11)

Rilsan® BUM 30 O

Suministrada por:

Arkema: High Performance Polymers

Polyamide 11 (PA11)

Rilsan® BUM 30 BLACK

Suministrada por:

Arkema: High Performance Polymers