Property | Temperature | Value | Condition | Testing Standard | Thickness |
---|---|---|---|---|---|
Density | 1.24 g/cm³ Show Supplier Material materials with Density of 1.24 g/cm³ | dry | ISO 1183 | ||
Moisture absorption | 23 °C | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | 50%RH | ISO 62 | 2 mm |
Mechanical
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elastic modulus | 3.2 GPa Show Supplier Material materials with Elastic modulus of 3.2 GPa | dry | ISO 527-2/1A | 1mm/min | |
Elongation | 17 % Show Supplier Material materials with Elongation of 17 % | dry | ISO 527-2/1A | 50mm/min | nominal | |
Elongation at yield | 10 % Show Supplier Material materials with Elongation at yield of 10 % | dry | ISO 527-2/1A | 50mm/min | |
Flexural modulus | 3 GPa Show Supplier Material materials with Flexural modulus of 3 GPa | dry | ISO 178 | 2mm/min | |
Flexural strength | 100 MPa Show Supplier Material materials with Flexural strength of 100 MPa | dry | ISO 178 | 2mm/min | |
Impact strength, Charpy notched | -30 °C | 4 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 4 kJ/m² | dry | ISO 179/1eA | |
23 °C | 4.5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 4.5 kJ/m² | dry | ISO 179/1eA | ||
Impact strength, Charpy unnotched | -30 °C | 97 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 97 kJ/m² | dry | ISO 179/1eU | |
23 °C | 96 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 96 kJ/m² | dry | ISO 179/1eU | ||
Yield strength | 73 MPa Show Supplier Material materials with Yield strength of 73 MPa | dry | ISO 527-2/1A | 50mm/min |
Thermal
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature | 70 °C Show Supplier Material materials with Heat deflection temperature of 70 °C | ISO 75/2Af | 1.80 MPa | ||
Melting point | 260 °C Show Supplier Material materials with Melting point of 260 °C | ISO 11357-1/-3 | 10°C/min | ||
Flammability | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 | Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3 |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Metal Detectable |