Impact strength, Izod notched, ASTM: 43 J/m

Quick Comparison

Poliamida

EXTEM™ Resin XH1015 - Europe

Suministrada por:

Sabic

Poliamida

EXTEM™ Resin XH1015 - Asia

Suministrada por:

Sabic

Poliamida

EXTEM™ Resin XH1015 - Americas

Suministrada por:

Sabic

Polietersulfona (PES)

LNP™ THERMOCOMP™ Compound JF003E

Suministrada por:

Sabic

Tereftalato de polibutileno (PBT)

LNP™ LUBRICOMP™ Compound WL001RZ

Suministrada por:

Sabic

Polyphenylene Sulfide (PPS)

LNP™ STAT-KON™ Compound OE002 - Asia

Suministrada por:

Sabic

Polyphenylene Sulfide (PPS)

LNP™ STAT-KON™ Compound OE002 - Americas

Suministrada por:

Sabic