LNP™ STAT-KON™ Compound OE002 - Americas

Want to keep this datasheet? Save it now in your required format

Description

LNP STAT-KON OE002 is a compound based on PPS - Linear resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

1.7 %

Show Supplier Material materials with Elongation of 1.7 %

ISO 527 | yield, 5 mm/min

Flexural strength

23.0 °C

148 MPa

Show Supplier Material materials with Flexural strength of 148 MPa

ISO 178

Impact strength, Izod notched

23.0 °C

2 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 2 kJ/m²

ISO 180/1A | 80*10*4, 23°C

Impact strength, Izod notched, ASTM

23.0 °C

43 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 43 J/m

ASTM D 256 | notched, 23°C

Impact strength, Izod unnotched, ASTM

23.0 °C

370 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 370 J/m

ASTM D 4812 | 23°C

Tensile strength

23.0 °C

96 MPa

Show Supplier Material materials with Tensile strength of 96 MPa

ISO 527 | break, 5 mm/min

Thermal

PropertyValueComment

Heat deflection temperature

122 °C

Show Supplier Material materials with Heat deflection temperature of 122 °C

Heat deflection temperature, 1.80 MPa

122 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 122 °C

ISO 75/Af | Flatw 80*10*4 sp=64mm

Technological properties

Property
Availability

Asia,Americas

Features

Super Strong (Carbon Fiber Filled), Electrically Conductive

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.