Impact strength, Izod notched, ASTM: 760 J/m

Quick Comparison

Policarbonato (PC)

LEXAN™ FR Resins LUX9610

Policarbonato (PC)

LEXAN™ Resin ML7682

Policarbonato (PC)

LEXAN™ Resin EM1210