LEXAN™ FR Resins LUX9610

Want to keep this datasheet? Save it now in your required format

Description

LEXAN LUX9610 is an injection moldable polycarbonate (PC) with an MVR (300°C/1.2kg) 7. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0@1.5mm rating. This is a UV stabilized, transparent grade with high optical clarity and impact resistance.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.2 g/cm³

Show Material materials with Density of 1.2 g/cm³

ISO 1183

Water absorption

23.0 °C

0.15 %

Show Material materials with Water absorption of 0.15 %

ISO 62 | 23°C, 50% RH

Water absorption, equilibrium

100.0 °C

0.58 %

Show Material materials with Water absorption, equilibrium of 0.58 %

ASTM D 570

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.23 GPa

Show Material materials with Elastic modulus of 2.23 GPa

ISO 527 | 1 mm/min

Elongation

23.0 °C

77 %

Show Material materials with Elongation of 77 %

ISO 527 | 50 mm/min

Elongation at yield

23.0 °C

6 %

Show Material materials with Elongation at yield of 6 %

ISO 527 | 50 mm/min

Flexural modulus

23.0 °C

2.25 GPa

Show Material materials with Flexural modulus of 2.25 GPa

ISO 178 | 2 mm/min

Flexural yield strength

23.0 °C

94 MPa

Show Material materials with Flexural yield strength of 94 MPa

ISO 178 | 2 mm/min

Hardness, Rockwell R

23.0 °C

118 [-]

Show Material materials with Hardness, Rockwell R of 118 [-]

ASTM D 785

Impact strength, Charpy notched

-30.0 °C

12 kJ/m²

Show Material materials with Impact strength, Charpy notched of 12 kJ/m²

ISO 179/1eA

23.0 °C

68 kJ/m²

Show Material materials with Impact strength, Charpy notched of 68 kJ/m²

ISO 179/1eA

Impact strength, Izod notched

-30.0 °C

11 kJ/m²

Show Material materials with Impact strength, Izod notched of 11 kJ/m²

ISO 180/1A

23.0 °C

70 kJ/m²

Show Material materials with Impact strength, Izod notched of 70 kJ/m²

ISO 180/1A

Unlock all property charts

Impact strength, Izod notched, ASTM

23.0 °C

760 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 760 J/m

ASTM D 256

Tensile strength

23.0 °C

58 MPa

Show Material materials with Tensile strength of 58 MPa

ISO 527 | 50 mm/min

Yield strength

23.0 °C

62 MPa

Show Material materials with Yield strength of 62 MPa

ISO 527 | 50 mm/min

Impact strength, Charpy unnotched

No Break @ 23,-30°C | ISO 179/1eU

Impact strength, Izod unnotched

No Break @ 23,-30°C| ISO 180/1U

Impact strength, Izod unnotched, ASTM

No break @ 23°C | ASTM D 4812

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

6.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 6.8E-5 1/K

ASTM E 831 | -40°C to 40°C

Coefficient of thermal expansion, transverse

23.0 °C

6.7E-5 1/K

Show Material materials with Coefficient of thermal expansion, transverse of 6.7E-5 1/K

ASTM E 831 | -40°C to 40°C

Heat deflection temperature, 1.80 MPa

125 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 125 °C

ISO 75/Af | 1.8 MPa

Relative temperature index, electrical

125 °C

Show Material materials with Relative temperature index, electrical of 125 °C

UL 746B

Relative temperature index, mechanical impact

115 °C

Show Material materials with Relative temperature index, mechanical impact of 115 °C

UL 746B

Relative temperature index, mechanical strength

125 °C

Show Material materials with Relative temperature index, mechanical strength of 125 °C

UL 746B

Specific heat capacity

23.0 °C

1260 J/(kg·K)

Show Material materials with Specific heat capacity of 1260 J/(kg·K)

ASTM C 351

Thermal conductivity

23.0 °C

0.2 W/(m·K)

Show Material materials with Thermal conductivity of 0.2 W/(m·K)

ASTM C177

Vicat softening temperature

145 °C

Show Material materials with Vicat softening temperature of 145 °C

ISO 306 | Rate B/120

Flammability

UL Recognized, 94V-0 Flame Class Rating | 1.5mm | UL 94

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

3 V

Show Material materials with Comparative tracking index of 3 V

UL 746A

Dielectric constant

23.0 °C

2.96 [-]

Show Material materials with Dielectric constant of 2.96 [-]

ASTM D 150 | at 1 MHz

Dielectric strength

23.0 °C

15 kV/mm

Show Material materials with Dielectric strength of 15 kV/mm

ASTM D 149 | in air, 3.2 mm

Dissipation factor

23.0 °C

0.01 [-]

Show Material materials with Dissipation factor of 0.01 [-]

ASTM D 150 | at 1 MHz

Optical

PropertyValueComment

Haze

1 %

Show Material materials with Haze of 1 %

SABIC method | 2mm

Refractive index

1.59 [-]

Show Material materials with Refractive index of 1.59 [-]

ISO 489

Rheological Properties

PropertyTemperatureValueComment

Melt volume-flow rate

7 cm³/10min

Show Material materials with Melt volume-flow rate of 7 cm³/10min

ISO 1133 | 300°C/1.2 kg

Shrinkage

23.0 °C

0.6 - 0.8 %

Show Material materials with Shrinkage of 0.6 - 0.8 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Air Cabin Interiors,Amusement Machine,ATM/Ticket Machine,Data Transfer,Displays,Document Handling,Enclosures,Heavy Vehicles,Individual Equiptment,LED Lighting,Non-LED Lighting,Personal Computing,Power Manangement,Wiring Devices

Processing methods

Drying Temperature: 120°C, Drying Time: 2-4hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 280-300°C, Nozzle Temperature: 270-290°C, Front - Zone 3 Temperature: 280-300°C, Middle - Zone 2 Temperature: 270-290°C, Rear - Zone 1 Temperature: 260-280°C, Hopper Temperature: 60-80°C, Mold Temperature: 80-100°C