Common features of Delrin® acetal resins include mechanical and physical properties such as high mechanical strength and rigidity, excellent fatigue and impact resistance, as well as resistance to moisture, gasoline, lubricants, solvents, and many other neutral chemicals. Delrin® acetal resins also have excellent dimensional stability and good electrical insulating characteristics. They are naturally resilient, self-lubricating, and available in a variety of colors and speciality grades. Delrin® acetal resin typically is used in demanding applications in the automotive, domestic appliances, sports, industrial engineering, electronics, and consumer goods industries.Delrin® 127UVE is a UV-stabilized high viscosity acetal homopolymer with very low VOC emissions, developed for applications in automotive interiors. Processing methods include injection molding.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.42 g/cm³

Show Material materials with Density of 1.42 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.9 GPa

Show Material materials with Elastic modulus of 2.9 GPa

ISO 527-1/-2

Elongation

23.0 °C

45 %

Show Material materials with Elongation of 45 %

ISO 527-1/-2

Elongation at yield

23.0 °C

25 %

Show Material materials with Elongation at yield of 25 %

ISO 527-1/-2

Flexural modulus

23.0 °C

2.8 GPa

Show Material materials with Flexural modulus of 2.8 GPa

ISO 178

Hardness, Rockwell M

23.0 °C

88.3 [-]

Show Material materials with Hardness, Rockwell M of 88.3 [-]

ISO 2039-2

Hardness, Rockwell R

23.0 °C

120 [-]

Show Material materials with Hardness, Rockwell R of 120 [-]

ISO 2039-2

Impact strength, Charpy notched

-6.0 °C

10 kJ/m²

Show Material materials with Impact strength, Charpy notched of 10 kJ/m²

ISO 179/1eA

23.0 °C

14 kJ/m²

Show Material materials with Impact strength, Charpy notched of 14 kJ/m²

ISO 179/1eA

Impact strength, Charpy unnotched

-6.0 °C

340 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 340 kJ/m²

ISO 179/1eU

23.0 °C

390 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 390 kJ/m²

ISO 179/1eU

Unlock all property charts

Impact strength, Izod notched

-30.0 °C

280 kJ/m²

Show Material materials with Impact strength, Izod notched of 280 kJ/m²

ISO 180/1U

Impact strength, Izod unnotched

23.0 °C

12 kJ/m²

Show Material materials with Impact strength, Izod unnotched of 12 kJ/m²

ISO 180/1A

Poisson's ratio

23.0 °C

0.37 [-]

Show Material materials with Poisson's ratio of 0.37 [-]

Yield strength

23.0 °C

71 MPa

Show Material materials with Yield strength of 71 MPa

ISO 527-1/-2

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.2E-4 1/K

Show Material materials with Coefficient of thermal expansion of 1.2E-4 1/K

ISO 11359-1/-2

Coefficient of thermal expansion, transverse

23.0 °C

1.1E-4 1/K

Show Material materials with Coefficient of thermal expansion, transverse of 1.1E-4 1/K

ISO 11359-1/-2

Heat deflection temperature, 0.45 MPa

159 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 159 °C

ISO 75-1/-2

Heat deflection temperature, 1.80 MPa

91 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 91 °C

ISO 75-1/-2

Melting point

178 °C

Show Material materials with Melting point of 178 °C

ISO 11357-1/-3 | 18°F/min

Vicat softening temperature

174 °C

Show Material materials with Vicat softening temperature of 174 °C

ISO 306 | 90°F, 2 lbf

Flammability

FMVSS Class: B -, Burning rate, Thickness 1 mm: 27 mm/min

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

2.5 g/10min

Show Material materials with Melt mass-flow rate of 2.5 g/10min

ISO 1133 | 190°C/2.16kg

Melt volume-flow rate

2.1 cm³/10min

Show Material materials with Melt volume-flow rate of 2.1 cm³/10min

ISO 1133

Shrinkage

23.0 °C

2.1 %

Show Material materials with Shrinkage of 2.1 %

ISO 294-4, 2577

Shrinkage, transverse

23.0 °C

1.9 %

Show Material materials with Shrinkage, transverse of 1.9 %

ISO 294-4, 2577

Technological properties

Property
Processing methods

Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 205°C, Min. melt temperature: 200°C, Max. melt temperature: 210°C, Mold Temperature Optimum: 90°C, Min. mold temperature: 80°C, Max. mold temperature: 100°C, Hold pressure range: 90-110MPa, Hold pressure time: 8s/mm