Kynar Flex® 2821-00

Alternative and trade names
PVDF
Want to keep this datasheet? Save it now in your required format

Description

Kynar Flex® resins are fluorinated thermoplastic copolymers.

Outstanding characteristics: chemical resistance, imperviousness to UV, high barrier properties, high purity, good mechanical and thermo-mechanical properties.

Kynar Flex® 2821 resin is the powder form of the Kynar Flex® 2820-20 resin. To be used as an additive in LLDPE to improve the extrusion rate.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.77 g/cm³

Show Supplier Material materials with Density of 1.77 g/cm³

ISO 1183

Limiting oxygen index

23.0 °C

42 %

Show Supplier Material materials with Limiting oxygen index of 42 %

ISO 4589-1/-2

Water absorption

23.0 °C

0.03 %

Show Supplier Material materials with Water absorption of 0.03 %

Sim. to ISO 62

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

0.7 GPa

Show Supplier Material materials with Elastic modulus of 0.7 GPa

ISO 527-1/-2

Elongation

23.0 °C

50 %

Show Supplier Material materials with Elongation of 50 %

min., ISO 527-1/-2, nominal

Elongation at yield

23.0 °C

15 %

Show Supplier Material materials with Elongation at yield of 15 %

ISO 527-1/-2

Yield strength

23.0 °C

27 MPa

Show Supplier Material materials with Yield strength of 27 MPa

ISO 527-1/-2

Impact strength, Charpy notched

No break @ 23°C, ISO 179/1eA

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.6E-4 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.6E-4 1/K

ISO 11359-1/-2

Glass transition temperature

-40 °C

Show Supplier Material materials with Glass transition temperature of -40 °C

ISO 11357-1/-2, 10°C/min

Heat deflection temperature, 1.80 MPa

48 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 48 °C

ISO 75-1/-2

Melting point

143 °C

Show Supplier Material materials with Melting point of 143 °C

ISO 11357-1/-3, 10°C/min

Relative temperature index, electrical

130 °C

Show Supplier Material materials with Relative temperature index, electrical of 130 °C

UL 746B

Relative temperature index, mechanical strength

130 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C

UL 746B

Specific heat capacity

23.0 °C

745 - 958 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 745 - 958 J/(kg·K)

DSC

Thermal decomposition in air

375 °C

Show Supplier Material materials with Thermal decomposition in air of 375 °C

TGA, 1% wt. loss

Thermal decomposition in nitrogen

410 °C

Show Supplier Material materials with Thermal decomposition in nitrogen of 410 °C

TGA, 1% wt. loss

Vicat softening temperature

76 °C

Show Supplier Material materials with Vicat softening temperature of 76 °C

ISO 306, 50°C/h 50N

Flammability

At thickness 0.8 mm IEC 60695-11-10: V-0 and yellow card available, 5V at thickness 1.5 mm IEC 60695-11-20: 5VB

Electrical

PropertyTemperatureValueComment

Dielectric constant, 1MHz

23.0 °C

6 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 6 [-]

IEC 60250

Dissipation factor, 100Hz

23.0 °C

0.06 [-]

Show Supplier Material materials with Dissipation factor, 100Hz of 0.06 [-]

IEC 60250

Dissipation factor, 1MHz

23.0 °C

0.23 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 0.23 [-]

IEC 60250

Volume resistivity

23.0 °C

2.00E+14 Ω·cm

Show Supplier Material materials with Volume resistivity of 2.00E+14 Ω·cm

IEC 60093

Rheological Properties

PropertyValueComment

Melt volume-flow rate

3 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 3 cm³/10min

ISO 1133, 230°C/5kg

Technological properties

Property
Application areas

Main applications:

  • corrosion protection in the chemical industry
  • coating (painting, co-extrusion)
  • off shore
  • wire and cable

    or