General
Property | Value | Comment |
---|---|---|
Density | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elastic modulus | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel | |||
Elongation | 12.6 % Show Material materials with Elongation of 12.6 % | Predicted Value, A200 | |||
14 % Show Material materials with Elongation of 14 % | Quenched and Tempered | ASTM A543 | Plate | A50 | |
17.1 % Show Material materials with Elongation of 17.1 % | Predicted Value, A80 | ||||
18.4 % Show Material materials with Elongation of 18.4 % | Predicted Value, Transverse | ||||
20.2 % Show Material materials with Elongation of 20.2 % | Predicted Value, A80 Transverse | ||||
20.5 % Show Material materials with Elongation of 20.5 % | Predicted Value | ||||
Poisson's ratio | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel | |||
Reduction of area | 43.5 % Show Material materials with Reduction of area of 43.5 % | Predicted Value, Transverse | |||
44.8 % Show Material materials with Reduction of area of 44.8 % | Predicted Value | ||||
Shear modulus | 79.5 GPa Show Material materials with Shear modulus of 79.5 GPa | Predicted Value | |||
Shear strength | 618.1 MPa Show Material materials with Shear strength of 618.1 MPa | Predicted Value | |||
Tensile strength | 725 - 860 MPa Show Material materials with Tensile strength of 725 - 860 MPa | Quenched and Tempered | ASTM A543 | Plate | |
Yield strength | 318.2 MPa Show Material materials with Yield strength of 318.2 MPa | Predicted Value, RP1 | |||
330.7 MPa Show Material materials with Yield strength of 330.7 MPa | Predicted Value, RP1 Transverse | ||||
332 MPa Show Material materials with Yield strength of 332 MPa | Predicted Value, RP05 | ||||
490 MPa Show Material materials with Yield strength of 490 MPa | Predicted Value, RP02 Transverse | ||||
495 MPa Show Material materials with Yield strength of 495 MPa | Predicted Value, Transverse | ||||
585 MPa Show Material materials with Yield strength of 585 MPa | Quenched and Tempered | ASTM A543 | Plate | ||
596.7 MPa Show Material materials with Yield strength of 596.7 MPa | Predicted Value, RP02 | ||||
663.5 MPa Show Material materials with Yield strength of 663.5 MPa | Predicted Value, RP002 |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 11.88 1/K Show Material materials with Coefficient of thermal expansion of 11.88 1/K | Predicted Value |
Specific heat capacity | 458.5 J/(kg·K) Show Material materials with Specific heat capacity of 458.5 J/(kg·K) | Predicted Value |
Thermal conductivity | 31.3 W/(m·K) Show Material materials with Thermal conductivity of 31.3 W/(m·K) | Predicted Value |
Electrical
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Carbon | 0.2 % Show Material materials with Carbon of 0.2 % | Quenched and Tempered | ASTM A543 | Plate |
Chromium | 1 - 1.9 % Show Material materials with Chromium of 1 - 1.9 % | Quenched and Tempered | ASTM A543 | Plate |
Manganese | 0.4 % Show Material materials with Manganese of 0.4 % | Quenched and Tempered | ASTM A543 | Plate |
Molybdenum | 0.2 - 0.65 % Show Material materials with Molybdenum of 0.2 - 0.65 % | Quenched and Tempered | ASTM A543 | Plate |
Nickel | 2.25 - 4 % Show Material materials with Nickel of 2.25 - 4 % | Quenched and Tempered | ASTM A543 | Plate |
Phosphorus | 0.02 % Show Material materials with Phosphorus of 0.02 % | Quenched and Tempered | ASTM A543 | Plate |
Silicon | 0.15 - 0.4 % Show Material materials with Silicon of 0.15 - 0.4 % | Quenched and Tempered | ASTM A543 | Plate |
Sulfur | 0.02 % Show Material materials with Sulfur of 0.02 % | Quenched and Tempered | ASTM A543 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |