Acero inoxidable austenítico
Sandvik 2RE10Suministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable austenítico
EN 10088-1 Grade X1CrNiMoN25-22-2 solution annealed (+AT)Acero inoxidable austenítico
Sandvik 7RE10Suministrada por:
Alleima (formerly Sandvik Materials Technology)Wrought Copper Nickel Silver Grade
BS NS106 Nickel SilverAcero inoxidable austenítico
EN 10088-1 Grade X1CrNi25-21 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X1CrNi25-21 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X1CrNiMoN25-22-2 solution annealed (+AT)Acero inoxidable austenítico
EN 10216-5 Grade X1CrNi25-21 solution annealed (+AT)Acero inoxidable austenítico
EN 10216-5 Grade X1CrNiMoN25-22-2 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X6CrNi25-20 solution annealed (+AT)Acero inoxidable austenítico
EN 10095 Grade X15CrNiSi25-21 solution annealed (+AT)Acero inoxidable austenítico
EN 10095 Grade X8CrNi25-21 solution annealed (+AT)Acero inoxidable austenítico
SEW 470 Grade X8CrNi25-21 solution annealed (+AT)Acero inoxidable austenítico
SEW 470 Grade X15CrNiSi25-21 solution annealed (+AT)Wrought Copper Nickel Silver Grade
EN 12166 Grade CuNi18Zn20 O60Acero inoxidable austenítico
SEW 400 Grade X1CrNi25-21 quenched (+Q)Wrought Copper Nickel Silver Grade
EN 12163 Grade CuNi18Zn20 R400Wrought Copper Nickel Silver Grade
EN 12164 Grade CuNi18Zn19Pb1 R420Wrought Copper Nickel Silver Grade
EN 1652 Grade CuNi18Zn20 R500Wrought Copper Nickel Silver Grade
EN 1652 Grade CuNi18Zn20 R580