Plane-Strain Fracture Toughnes: 41.7 - 50.5 MPa·√m

Quick Comparison

2000 Serie

EN 573-3 Grade AW-2024 T3

Suministrada por:

1 proveedor Matmatch

2000 Serie

EN 573-3 Grade AW-2024 T3

Suministrada por:

1 proveedor Matmatch

7000 Serie

WL 3.4354-1 Grade 3.4354 T74

Suministrada por:

1 proveedor Matmatch

Ductile (Nodular) Cast Iron

EN 1564 Grade GJS-1400-1 cast condition