General
Property | Value | Comment |
---|---|---|
Density | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elastic modulus | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel | |||
Elongation | 18.8 % Show Material materials with Elongation of 18.8 % | Predicted Value, A80 | |||
19.0 % Show Material materials with Elongation of 19.0 % | Predicted Value, Transverse | ||||
19.8 % Show Material materials with Elongation of 19.8 % | Predicted Value, A80 Transverse | ||||
21 % Show Material materials with Elongation of 21 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate | A200 | |
24.2 % Show Material materials with Elongation of 24.2 % | Predicted Value | ||||
25 % Show Material materials with Elongation of 25 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate | A50 | |
Poisson's ratio | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel | |||
Reduction of area | 42.9 % Show Material materials with Reduction of area of 42.9 % | Predicted Value | |||
43.0 % Show Material materials with Reduction of area of 43.0 % | Predicted Value, Transverse | ||||
Shear modulus | 79.4 GPa Show Material materials with Shear modulus of 79.4 GPa | Predicted Value | |||
Shear strength | 503.5 MPa Show Material materials with Shear strength of 503.5 MPa | Predicted Value | |||
Tensile strength | 415 - 550 MPa Show Material materials with Tensile strength of 415 - 550 MPa | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 11.83 1/K Show Material materials with Coefficient of thermal expansion of 11.83 1/K | Predicted Value |
Specific heat capacity | 457.4 J/(kg·K) Show Material materials with Specific heat capacity of 457.4 J/(kg·K) | Predicted Value |
Thermal conductivity | 39.96 W/(m·K) Show Material materials with Thermal conductivity of 39.96 W/(m·K) | Predicted Value |
Electrical
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Carbon | 0.21 % Show Material materials with Carbon of 0.21 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate |
Manganese | 0.6 - 0.9 % Show Material materials with Manganese of 0.6 - 0.9 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate |
Phosphorus | 0.025 % Show Material materials with Phosphorus of 0.025 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate |
Silicon | 0.15 - 0.4 % Show Material materials with Silicon of 0.15 - 0.4 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |