General
Property | Value | Comment |
---|---|---|
Density | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Elastic modulus | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel | ||
Elongation | 17.5 % Show Material materials with Elongation of 17.5 % | Predicted Value, A80 | ||
18 % Show Material materials with Elongation of 18 % | ASTM A573 | Plate | A200 | |
18.1 % Show Material materials with Elongation of 18.1 % | Predicted Value, Transverse | |||
19.3 % Show Material materials with Elongation of 19.3 % | Predicted Value, A80 Transverse | |||
21 % Show Material materials with Elongation of 21 % | ASTM A573 | Plate | A50 | |
23.1 % Show Material materials with Elongation of 23.1 % | Predicted Value | |||
Poisson's ratio | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel | ||
Reduction of area | 43.6 % Show Material materials with Reduction of area of 43.6 % | Predicted Value, Transverse | ||
43.8 % Show Material materials with Reduction of area of 43.8 % | Predicted Value | |||
Shear modulus | 79.4 GPa Show Material materials with Shear modulus of 79.4 GPa | Predicted Value | ||
Shear strength | 534.7 MPa Show Material materials with Shear strength of 534.7 MPa | Predicted Value | ||
Tensile strength | 485 - 620 MPa Show Material materials with Tensile strength of 485 - 620 MPa | ASTM A573 | Plate | |
Yield strength | 265.5 MPa Show Material materials with Yield strength of 265.5 MPa | Predicted Value, RP1 | ||
288.6 MPa Show Material materials with Yield strength of 288.6 MPa | Predicted Value, RP05 | |||
290 MPa Show Material materials with Yield strength of 290 MPa | ASTM A573 | Plate | ||
315.9 MPa Show Material materials with Yield strength of 315.9 MPa | Predicted Value, RP1 Transverse | |||
329 MPa Show Material materials with Yield strength of 329 MPa | Predicted Value, Transverse | |||
372.1 MPa Show Material materials with Yield strength of 372.1 MPa | Predicted Value, RP02 | |||
411.9 MPa Show Material materials with Yield strength of 411.9 MPa | Predicted Value, RP002 | |||
484.2 MPa Show Material materials with Yield strength of 484.2 MPa | Predicted Value, RP02 Transverse |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 12.1 1/K Show Material materials with Coefficient of thermal expansion of 12.1 1/K | Predicted Value |
Specific heat capacity | 459.7 J/(kg·K) Show Material materials with Specific heat capacity of 459.7 J/(kg·K) | Predicted Value |
Thermal conductivity | 38.44 W/(m·K) Show Material materials with Thermal conductivity of 38.44 W/(m·K) | Predicted Value |
Electrical
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Carbon | 0.27 % Show Material materials with Carbon of 0.27 % | ASTM A573 | Plate |
Manganese | 0.85 - 1.2 % Show Material materials with Manganese of 0.85 - 1.2 % | ASTM A573 | Plate |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % | ASTM A573 | Plate |
Silicon | 0.15 - 0.4 % Show Material materials with Silicon of 0.15 - 0.4 % | ASTM A573 | Plate |
Sulfur | 0.03 % Show Material materials with Sulfur of 0.03 % | ASTM A573 | Plate |