Specific Electrical conductivity: 20 % IACS

Quick Comparison

Wrought Copper High Copper Alloy

ASTM B196 Grade C17200 TB00

Wrought Copper High Copper Alloy

EN 1652 Grade C17200 TF00

Wrought Copper High Copper Alloy

Alloy 190 TM00 (C17200)

Suministrada por:

Materion Brush GmbH

Wrought Copper High Copper Alloy

Alloy 190 TM01 (C17200)

Suministrada por:

Materion Brush GmbH

Wrought Copper High Copper Alloy

Alloy 190 TM02 (C17200)

Suministrada por:

Materion Brush GmbH

Wrought Copper High Copper Alloy

Alloy 190 TM04 (C17200)

Suministrada por:

Materion Brush GmbH

Wrought Copper High Copper Alloy

Alloy 190 TM05 (C17200)

Suministrada por:

Materion Brush GmbH

Wrought Copper High Copper Alloy

Alloy 190 TM06 (C17200)

Suministrada por:

Materion Brush GmbH

Wrought Copper High Copper Alloy

Alloy 190 TM08 (C17200)

Suministrada por:

Materion Brush GmbH

Wrought Copper High Copper Alloy

Alloy 290 TM02 (C17200)

Suministrada por:

Materion Brush GmbH

Wrought Copper High Copper Alloy

Alloy 290 TM03 (C17200)

Suministrada por:

Materion Brush GmbH

Wrought Copper High Copper Alloy

Alloy 290 TM04 (C17200)

Suministrada por:

Materion Brush GmbH

Wrought Copper High Copper Alloy

Alloy 290 TM06 (C17200)

Suministrada por:

Materion Brush GmbH

Wrought Copper High Copper Alloy

Alloy 290 TM08 (C17200)

Suministrada por:

Materion Brush GmbH

Bronce fosforado

JIS C5111 Harada

Suministrada por:

HARADA METAL INDUSTRY CO., LTD.

Wrought Copper High Copper Alloy

AMPCOLOY® 83 Sand castings

Suministrada por:

AMPCO METAL

Wrought Copper High Copper Alloy

EtchMetᵀᴹ TM20 (C17200) Strip

Suministrada por:

Materion Brush GmbH

Wrought Copper High Copper Alloy

EtchMetᵀᴹ TM10 (C17200) Strip

Suministrada por:

Materion Brush GmbH

Wrought Copper High Copper Alloy

EN 12166 Grade CuBe2Pb R1150

Wrought Copper High Copper Alloy

EN 12166 Grade CuBe2Pb R1300
Página 1 de 3