EtchMetᵀᴹ TM10 (C17200) Strip

Want to keep this datasheet? Save it now in your required format

Description

EtchMet alloy is a material that is tailor made for the springs in voice coil motors and optical image stabilization systems common in smart phone cameras. These devices have a relatively large mass (lense) suspended by extremely small, thin springs. The small size of the springs requires very high strength material to withstand shock loads when the phone is dropped or deliberately tapped against an NFC reader. Therefore, the springs must be made from a very robust material. Furthermore, the lack of a damping mechanism makes high spring stiffness important to combat vibration. EtchMet alloy provides a number of advantages that make it the ideal material for this application:


  • It has a uniform elastic modulus across all thicknesses/diameters and from product form to product form. This provides consistent stiffness and damping behavior which makes spring calculations easy.
  • It has a very high resilience allowing it to withstand impact loads without fracturing or permanently deforming.
  • It has high fatigue strength to withstand many drops and actuation cycles.
  • It has a uniform, primarily single-phase microstructure, which photochemically machines easily and cleanly for uniform edges free of stress risers.
  • It is supplied fully precipitation hardened so no further heat treatment is required.
  • It solders and welds readily.
  • EtchMet strip is inherently flat with minimal coil set, which helps with alignment during photochemical machining.
  • This material data has been provided by Materion Brush GmbH.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValue

    Density

    23.0 °C

    8.36 g/cm³

    Show Supplier Material materials with Density of 8.36 g/cm³

    Dimension

    PropertyValue

    Thickness

    0.03 - 0.05 mm

    Show Supplier Material materials with Thickness of 0.03 - 0.05 mm

    Width

    1.27 - 406.5 mm

    Show Supplier Material materials with Width of 1.27 - 406.5 mm

    Mechanical

    PropertyTemperatureValueComment

    Elastic modulus

    23.0 °C

    131 GPa

    Show Supplier Material materials with Elastic modulus of 131 GPa

    Elongation

    23.0 °C

    3 %

    Show Supplier Material materials with Elongation of 3 %

    min.

    Hardness, Vickers

    23.0 °C

    325 [-]

    Show Supplier Material materials with Hardness, Vickers of 325 [-]

    min.

    Tensile strength

    23.0 °C

    1200 MPa

    Show Supplier Material materials with Tensile strength of 1200 MPa

    min.

    Yield strength Rp0.2

    23.0 °C

    1103 MPa

    Show Supplier Material materials with Yield strength Rp0.2 of 1103 MPa

    min.

    Thermal

    PropertyTemperatureValue

    Coefficient of thermal expansion

    23.0 °C

    1.75E-5 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 1.75E-5 1/K

    Thermal conductivity

    23.0 °C

    105 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 105 W/(m·K)

    Electrical

    PropertyTemperatureValue

    Electrical resistivity

    23.0 °C

    6.2E-6 - 1.01E-5 Ω·m

    Show Supplier Material materials with Electrical resistivity of 6.2E-6 - 1.01E-5 Ω·m

    Specific Electrical conductivity

    17 - 28 % IACS

    Show Supplier Material materials with Specific Electrical conductivity of 17 - 28 % IACS

    Magnetic

    PropertyTemperatureValueComment

    Relative magnetic permeability

    23.0 °C

    1 [-]

    Show Supplier Material materials with Relative magnetic permeability of 1 [-]

    max.

    Technological properties

    Property
    Application areas

    EtchMet alloy is a material that is tailor made for the springs in voice coil motors and optical image stabilization systems common in smart phone cameras.