Conductividad térmica: 2.1 W/(m·K)

Quick Comparison

Other Polyamide (PA)

Stanyl® TC168 (NC239B)

Suministrada por:

DSM Engineering Materials

Other Polyamide (PA)

Stanyl® TC170

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TC551

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TC502

Suministrada por:

DSM Engineering Materials