General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.42 g/cm³ Show Supplier Material materials with Density of 1.42 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2 % Show Supplier Material materials with Moisture absorption of 2 % | dry | Sim. to ISO 62 |
Mechanical
Property | Value | Condition | Testing Standard |
---|---|---|---|
Elastic modulus | 9 GPa Show Supplier Material materials with Elastic modulus of 9 GPa | dry | ISO 527-1/-2 |
Elongation | 1.1 % Show Supplier Material materials with Elongation of 1.1 % | dry | ISO 527-1/-2 |
Tensile strength | 65 MPa Show Supplier Material materials with Tensile strength of 65 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Coefficient of thermal expansion | 2.5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel |
3.5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 3.5e-07 1/K | dry | ISO 11359-1/-2 | Normal | |
Glass transition temperature | 75 °C Show Supplier Material materials with Glass transition temperature of 75 °C | dry | ISO 11357-1/-2 | 10°C/min |
Melting point | 295 °C Show Supplier Material materials with Melting point of 295 °C | dry | ISO 11357-1/-3 | 10°C/min |
Thermal conductivity | 2.1 W/(m·K) Show Supplier Material materials with Thermal conductivity of 2.1 W/(m·K) | dry | ASTM E1461 | through plane |
14.0 W/(m·K) Show Supplier Material materials with Thermal conductivity of 14.0 W/(m·K) | dry | ASTM E1461 | in plane |
Electrical
Property | Value | Condition | Testing Standard |
---|---|---|---|
Surface resistivity | 1e+07 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+07 Ω/sq | conditioned | IEC 62631-3-2 |
Volume resistivity | 10000 Ω·cm Show Supplier Material materials with Volume resistivity of 10000 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | LED Headlight Lighting Modules and Lensholders, Cover Electric Control Unit | |
Fillers | 15% Glass Fiber |