General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.87 g/cm³ Show Supplier Material materials with Density of 1.87 g/cm³ | dry | ISO 1183 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 14 GPa Show Supplier Material materials with Elastic modulus of 14 GPa | dry | ISO 527-1/-2 | |
Elongation | 1.6 % Show Supplier Material materials with Elongation of 1.6 % | dry | ISO 527-1/-2 | |
Impact strength, Charpy notched | -30 °C | 7.5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 7.5 kJ/m² | dry | ISO 179/1eA |
23 °C | 8 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 8 kJ/m² | dry | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 24 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 24 kJ/m² | dry | ISO 179/1eU |
23 °C | 24 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 24 kJ/m² | dry | ISO 179/1eU | |
Tensile strength | 115 MPa Show Supplier Material materials with Tensile strength of 115 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 2.1e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.1e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
2.5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Heat deflection temperature | 214 °C Show Supplier Material materials with Heat deflection temperature of 214 °C | dry | ISO 75-1/-2 | 2 MPa | |
Melting point | 290 °C Show Supplier Material materials with Melting point of 290 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Thermal conductivity | 0.9 W/(m·K) Show Supplier Material materials with Thermal conductivity of 0.9 W/(m·K) | dry | ASTM E1461 | through plane | |
2.1 W/(m·K) Show Supplier Material materials with Thermal conductivity of 2.1 W/(m·K) | dry | ASTM E1461 | in plane |
Electrical
Property | Value | Condition | Testing Standard |
---|---|---|---|
Comparative tracking index | 300 V Show Supplier Material materials with Comparative tracking index of 300 V | dry | IEC 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Heat Sinks in LED Lamps | |
Certifications | Yellow Card Available | |
Fillers | 20% Glass Fiber |