Acero bajo en carbono
EN 10025-2 Grade S275J0 normalized or normalized formed (+N)Suministrada por:
1 proveedor Matmatch
7000 Serie
AA Standards Grade 7075 T7351Acero bajo en carbono
EN 10217-3 Grade WStE 355 normalized or normalized formed (+N)Acero bajo en carbono
DIN 17179 Grade WStE 355 normalized or normalized formed (+N)Acero bajo en carbono
DIN 1628 Grade St 52.4 normalized or normalized formed (+N)Acero bajo en carbono
EN 10216-3 Grade P355NH normalized or normalized formed (+N)2000 Serie
WL 3.1924-1 Grade 3.1924 T651Acero bajo en carbono
EN 10217-3 Grade EStE 355 normalized or normalized formed (+N)Acero bajo en carbono
EN 10217-3 Grade StE 355 normalized or normalized formed (+N)Acero bajo en carbono
EN 10217-3 Grade TStE 355 normalized or normalized formed (+N)Acero bajo en carbono
EN 10025 Grade S355J2G3 normalized or normalized formed (+N)Acero bajo en carbono
EN 10025 Grade S355K2G3 normalized or normalized formed (+N)Acero bajo en carbono
DIN 17125 Grade StE 355 normalized or normalized formed (+N)Acero bajo en carbono
DIN 17125 Grade EStE 355 normalized or normalized formed (+N)