Description

Naturally hard AlMg alloy. The alloy is food safe.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey,Aludium.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueConditionRelated StandardsShape

Density

2.65 g/cm³

Show Material materials with Density of 2.65 g/cm³

H48

EN 573-3, EN 1396, EN 541

Strip, Sheet, Plate

2.65 g/cm³

Show Material materials with Density of 2.65 g/cm³

H48

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

20.0 °C

2.64 g/cm³

Show Material materials with Density of 2.64 g/cm³

H48

EN 573-3

Sheet, Strip

Dimension

PropertyValueConditionRelated StandardsThicknessShape

Thickness

0.2 mm

Show Material materials with Thickness of 0.2 mm

H48

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

0.2 mm

Coil, Sheet

0.35 mm

Show Material materials with Thickness of 0.35 mm

H48

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

0.35 mm

Coil, Sheet

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

H48

EN 573-3, EN 1396, EN 541

Strip, Sheet, Plate

71.0 GPa

Show Material materials with Elastic modulus of 71.0 GPa

H48

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

Hardness, HBW

114 [-]

Show Material materials with Hardness, HBW of 114 [-]

H48

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 5000 Series Aluminium

Shear modulus

20.0 °C

27.0 GPa

Show Material materials with Shear modulus of 27.0 GPa

H48

EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Sheet, Strip, Coil, Sheet

Tensile strength

330.0 MPa

Show Material materials with Tensile strength of 330.0 MPa

H48

EN 573-3, EN 1396

Strip, Sheet, Plate

380 MPa

Show Material materials with Tensile strength of 380 MPa

H48

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

20.0 °C

330.0 MPa

Show Material materials with Tensile strength of 330.0 MPa

H48

EN 573-3

Sheet, Strip

Transverse

20.0 °C

330.0 MPa

Show Material materials with Tensile strength of 330.0 MPa

H48

EN 573-3

Sheet, Strip

20.0 °C

355.0 - 400.0 MPa

Show Material materials with Tensile strength of 355.0 - 400.0 MPa

H48

EN 573-3, EN 541

Sheet, Strip, Plate

Yield strength

300.0 MPa

Show Material materials with Yield strength of 300.0 MPa

H48

EN 573-3, EN 1396

Strip, Sheet, Plate

RP02

320 MPa

Show Material materials with Yield strength of 320 MPa

H48

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

20.0 °C

300.0 MPa

Show Material materials with Yield strength of 300.0 MPa

H48

EN 573-3

Sheet, Strip

RP02 Transverse

20.0 °C

300.0 MPa

Show Material materials with Yield strength of 300.0 MPa

H48

EN 573-3

Sheet, Strip

RP02

20.0 °C

310.0 - 350.0 MPa

Show Material materials with Yield strength of 310.0 - 350.0 MPa

H48

EN 573-3, EN 541

Sheet, Strip, Plate

RP02

Thermal

PropertyTemperatureValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

20 °C

2.3199999999999998e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.3199999999999998e-05 1/K

H48

EN 573-3, EN 1396, EN 541

Strip, Sheet, Plate

100 °C

2.3199999999999998e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.3199999999999998e-05 1/K

H48

EN 573-3, EN 1396, EN 541

Strip, Sheet, Plate

100 °C

0.000024 1/K

Show Material materials with Coefficient of thermal expansion of 0.000024 1/K

H48

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

20-100°C

Max service temperature

150.0 °C

Show Material materials with Max service temperature of 150.0 °C

Typical for Wrought 5000 Series Aluminium

Melting point

577.0 - 638.0 °C

Show Material materials with Melting point of 577.0 - 638.0 °C

H48

EN 573-3, EN 1396, EN 541

Strip, Sheet, Plate

Specific heat capacity

20.0 °C

900.0 J/(kg·K)

Show Material materials with Specific heat capacity of 900.0 J/(kg·K)

H48

EN 573-3

Sheet, Strip

Thermal conductivity

121 W/(m·K)

Show Material materials with Thermal conductivity of 121 W/(m·K)

H48

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

123 W/(m·K)

Show Material materials with Thermal conductivity of 123 W/(m·K)

H48

EN 573-3, EN 1396, EN 541

Strip, Sheet, Plate

20.0 °C

140.0 W/(m·K)

Show Material materials with Thermal conductivity of 140.0 W/(m·K)

H48

EN 573-3

Sheet, Strip

Electrical

PropertyTemperatureValueConditionRelated StandardsShape

Electrical conductivity

18000000.0 S/m

Show Material materials with Electrical conductivity of 18000000.0 S/m

H48

EN 573-3, EN 1396, EN 541

Strip, Sheet, Plate

20.0 °C

19000000.0 S/m

Show Material materials with Electrical conductivity of 19000000.0 S/m

H48

EN 573-3

Sheet, Strip

Electrical resistivity

5.56e-08 Ω·m

Show Material materials with Electrical resistivity of 5.56e-08 Ω·m

H48

EN 573-3, EN 1396, EN 541

Strip, Sheet, Plate

5.6e-08 Ω·m

Show Material materials with Electrical resistivity of 5.6e-08 Ω·m

H48

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

Chemical properties

PropertyValueConditionRelated StandardsShape

Chromium

0.1 %

Show Material materials with Chromium of 0.1 %

H48

EN 573-3, EN 1396, EN 541

Sheet, Strip, Plate

0.1 %

Show Material materials with Chromium of 0.1 %

H48

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

Copper

0.15 %

Show Material materials with Copper of 0.15 %

H48

EN 573-3, EN 1396, EN 541

Sheet, Strip, Plate

0.15 %

Show Material materials with Copper of 0.15 %

H48

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

Iron

0.35 %

Show Material materials with Iron of 0.35 %

H48

EN 573-3

Sheet, Strip

0.35 %

Show Material materials with Iron of 0.35 %

H48

EN 573-3, EN 1396, EN 541, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Strip, Sheet, Plate, Coil, Sheet

Magnesium

4.0 - 5.0 %

Show Material materials with Magnesium of 4.0 - 5.0 %

H48

EN 573-3, EN 1396, EN 541, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Sheet, Strip, Plate, Coil, Sheet

Manganese

0.2 - 0.5 %

Show Material materials with Manganese of 0.2 - 0.5 %

H48

EN 573-3, EN 1396, EN 541, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Sheet, Strip, Plate, Coil, Sheet

Other

0.05 - 0.15 %

Show Material materials with Other of 0.05 - 0.15 %

H48

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

Silicon

0.2 %

Show Material materials with Silicon of 0.2 %

H48

EN 573-3, EN 1396, EN 541

Sheet, Strip, Plate

0.2 %

Show Material materials with Silicon of 0.2 %

H48

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

Titanium

0.1 %

Show Material materials with Titanium of 0.1 %

H48

EN 573-3, EN 1396, EN 541

Sheet, Strip, Plate

0.1 %

Show Material materials with Titanium of 0.1 %

H48

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

Zinc

0.25 %

Show Material materials with Zinc of 0.25 %

H48

EN 573-3, EN 1396, EN 541

Sheet, Strip, Plate

0.25 %

Show Material materials with Zinc of 0.25 %

H48

EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541

Coil, Sheet

Technological properties

Property
Anodizing

decorative: sufficient, Protective: good

Application areas

Wind energy: Nacelle coverings, rotor hub, stairs; Components: Heat shields, Access hatches, Spoilers, General tranportation

Brazing

hard brazing (with flux/ without flux): sufficient to not suitable / poor, friction soldering: acceptable, soft brazing with flux: poor

Corrosion properties

Seawater: very good, weathering: very good

Welding

Good

Workability

Bending / Spinning (cold): good / sufficient, Impact extrusion (cold): sufficient, Deep drawing / upsetting (Condition) good (O) / acceptable (O)