General
Property | Value | Comment |
---|---|---|
Density | 2.75 - 2.84 g/cm³ Show Material materials with Density of 2.75 - 2.84 g/cm³ | Typical for Wrought 2000 Series Aluminium |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastic modulus | 70.0 - 73.0 GPa Show Material materials with Elastic modulus of 70.0 - 73.0 GPa | Typical for Wrought 2000 Series Aluminium | ||||
Hardness, Brinell | 20.0 °C | 125.0 [-] Show Material materials with Hardness, Brinell of 125.0 [-] | T651 | WL 3.1924-1 | Plate | Transverse |
20.0 °C | 125.0 [-] Show Material materials with Hardness, Brinell of 125.0 [-] | T651 | WL 3.1924-1 | Rod | ||
Plane-Strain Fracture Toughnes | 20.0 °C | 17.7 - 21.2 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 17.7 - 21.2 MPa·√m | T651 | WL 3.1924-1 | ||
20.0 °C | 17.7 - 19.3 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 17.7 - 19.3 MPa·√m | T651 | WL 3.1924-1 | |||
20.0 °C | 17.7 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 17.7 MPa·√m | T651 | WL 3.1924-1 | |||
20.0 °C | 19.3 - 21.2 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 19.3 - 21.2 MPa·√m | T651 | WL 3.1924-1 | |||
20.0 °C | 19.3 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 19.3 MPa·√m | T651 | WL 3.1924-1 | |||
20.0 °C | 21.2 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 21.2 MPa·√m | T651 | WL 3.1924-1 | |||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 2000 Series Aluminium | ||||
Shear modulus | 26.0 - 27.5 GPa Show Material materials with Shear modulus of 26.0 - 27.5 GPa | Typical for Wrought 2000 Series Aluminium | ||||
Tensile strength | 20.0 °C | 390.0 MPa Show Material materials with Tensile strength of 390.0 MPa | T651 | WL 3.1924-1 | Plate | Transverse |
20.0 °C | 400.0 MPa Show Material materials with Tensile strength of 400.0 MPa | T651 | WL 3.1924-1 | Plate | Transverse | |
20.0 °C | 405.0 MPa Show Material materials with Tensile strength of 405.0 MPa | T651 | WL 3.1924-1 | Plate | Transverse | |
20.0 °C | 410.0 MPa Show Material materials with Tensile strength of 410.0 MPa | T651 | WL 3.1924-1 | Plate | Transverse | |
20.0 °C | 420.0 MPa Show Material materials with Tensile strength of 420.0 MPa | T651 | WL 3.1924-1 | Plate | Transverse | |
20.0 °C | 420.0 MPa Show Material materials with Tensile strength of 420.0 MPa | T651 | WL 3.1924-1 | Rod | ||
20.0 °C | 430.0 MPa Show Material materials with Tensile strength of 430.0 MPa | T651 | WL 3.1924-1 | Plate | Transverse | |
Yield strength | 20.0 °C | 335.0 - 375.0 MPa Show Material materials with Yield strength of 335.0 - 375.0 MPa | T651 | WL 3.1924-1 | ||
20.0 °C | 340.0 MPa Show Material materials with Yield strength of 340.0 MPa | T651 | WL 3.1924-1 | Plate | RP02 Transverse | |
20.0 °C | 350.0 MPa Show Material materials with Yield strength of 350.0 MPa | T651 | WL 3.1924-1 | Plate | RP02 Transverse | |
20.0 °C | 350.0 MPa Show Material materials with Yield strength of 350.0 MPa | T651 | WL 3.1924-1 | Rod | RP02 | |
20.0 °C | 370.0 MPa Show Material materials with Yield strength of 370.0 MPa | T651 | WL 3.1924-1 | Plate | RP02 Transverse | |
20.0 °C | 375.0 MPa Show Material materials with Yield strength of 375.0 MPa | T651 | WL 3.1924-1 | Plate | RP02 Transverse | |
20.0 °C | 380.0 MPa Show Material materials with Yield strength of 380.0 MPa | T651 | WL 3.1924-1 | Plate | RP02 Transverse | |
20.0 °C | 390.0 MPa Show Material materials with Yield strength of 390.0 MPa | T651 | WL 3.1924-1 | Plate | RP02 Transverse |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 1.6e-05 - 2.4e-05 1/K Show Material materials with Coefficient of thermal expansion of 1.6e-05 - 2.4e-05 1/K | Typical for Wrought 2000 Series Aluminium |
Melting point | 500.0 - 650.0 °C Show Material materials with Melting point of 500.0 - 650.0 °C | Typical for Wrought 2000 Series Aluminium |
Specific heat capacity | 816.0 - 963.0 J/(kg·K) Show Material materials with Specific heat capacity of 816.0 - 963.0 J/(kg·K) | Typical for Wrought 2000 Series Aluminium |
Thermal conductivity | 112.0 - 251.0 W/(m·K) Show Material materials with Thermal conductivity of 112.0 - 251.0 W/(m·K) | Typical for Wrought 2000 Series Aluminium |
Electrical
Property | Value | Comment |
---|---|---|
Electrical conductivity | 18000000.0 - 30000000.0 S/m Show Material materials with Electrical conductivity of 18000000.0 - 30000000.0 S/m | Typical for Wrought 2000 Series Aluminium |
Electrical resistivity | 3.4e-08 - 6e-08 Ω·m Show Material materials with Electrical resistivity of 3.4e-08 - 6e-08 Ω·m | Typical for Wrought 2000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Copper | 1.8 - 2.7 % Show Material materials with Copper of 1.8 - 2.7 % | T651 | WL 3.1924-1 | Plate, Rod |
Iron | 0.9 - 1.4 % Show Material materials with Iron of 0.9 - 1.4 % | T651 | WL 3.1924-1 | Plate, Rod |
Magnesium | 1.2 - 1.8 % Show Material materials with Magnesium of 1.2 - 1.8 % | T651 | WL 3.1924-1 | Plate, Rod |
Manganese | 0.2 Show Material materials with Manganese of 0.2 | T651 | WL 3.1924-1 | Plate, Rod |
Nickel | 0.8 - 1.4 % Show Material materials with Nickel of 0.8 - 1.4 % | T651 | WL 3.1924-1 | Plate, Rod |
Silicon | 0.15 - 0.25 % Show Material materials with Silicon of 0.15 - 0.25 % | T651 | WL 3.1924-1 | Plate, Rod |
Titanium | 0.2 Show Material materials with Titanium of 0.2 | T651 | WL 3.1924-1 | Plate, Rod |
Zinc | 0.1 Show Material materials with Zinc of 0.1 | T651 | WL 3.1924-1 | Plate, Rod |
Technological properties
Property | ||
---|---|---|
Workability | Moderate Workability |