Límite elástico Rp 0,2: 507 MPa

Quick Comparison

Wrought Copper High Copper Alloy

ASTM B196 Grade C17200 TB00

Wrought Copper High Copper Alloy

ASTM B194 Grade C17200 TD04

Wrought Copper High Copper Alloy

EN 1652 Grade C17200 TF00

Wrought Copper High Copper Alloy

ASTM B643 Grade C17200 TH04

Wrought Copper High Copper Alloy

ASTM B534 Grade C17500 TD04

Wrought Copper High Copper Alloy

ASTM B534 Grade C17510 TD04

Wrought Copper High Copper Alloy

ASTM B197 Grade C17300 TH04

Wrought Copper Nickel Grade

BrushForm® 158 Strip TD01 (C72900)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 96 TM00 Strip (C72700)

Suministrada por:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 96 TM02 Strip (C72700)

Suministrada por:

Materion Brush GmbH

Wrought Copper Bronze Silicon Bronze

COLSIBRO® Copper Alloy