Acero inoxidable austenítico
ASTM A193 Grade B8M2 Class 2B, Carbide solution treated and strain hardened; M48 and underAcero inoxidable austenítico
ASTM A320 Grade B8P Class 2, Carbide Solution Treated and Strain HardenedAcero inoxidable austenítico
ASTM A320 Grade B8T Class 2, Carbide Solution Treated and Strain HardenedAcero inoxidable austenítico
ASTM A320 Grade B8C Class 2, Carbide Solution Treated and Strain HardenedAcero inoxidable austenítico
ASTM A320 Grade B8F Class 2, Carbide Solution Treated and Strain HardenedAcero inoxidable austenítico
ASTM A320 Grade B8M Class 2, Carbide Solution Treated and Strain HardenedAcero inoxidable martensítico
ASTM A487 Grade CA6NM Class B, Heat-TreatedAcero inoxidable martensítico
ASTM A487 Grade CA15 Class D, Heat-TreatedAcero inoxidable martensítico
ASTM A487 Grade CA6NM Class A, Heat-TreatedAcero inoxidable martensítico
ASTM A487 Grade 7 Class A, Heat-TreatedNickel Chromium Molybdenum Steel
ASTM A372 Grade L Liquid Quenched and Tempered, or Normalized followed by Liquid Quench and TemperNickel Molybdenum Steel
ASTM A487 Grade 11 Class B, Heat-TreatedChromium Molybdenum Steel
ASTM A372 Grade J Class 90, Liquid Quenched and Tempered, or Normalized followed by Liquid Quench and TemperNickel Chromium Molybdenum Steel
ASTM A487 Grade 14 Class A, Heat-TreatedNickel Chromium Molybdenum Steel
ASTM A487 Grade 10 Class B, Heat-TreatedNickel Chromium Molybdenum Steel
ASTM A487 Grade 12 Class B, Heat-TreatedNickel Chromium Molybdenum Steel
ASTM A487 Grade 13 Class B, Heat-TreatedNickel Chromium Molybdenum Steel
ASTM A710 Grade A, Class 1 As-rolled and precipitation heat treated