General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 20.0 °C | 7.6 - 7.7 g/cm³ Show Material materials with Density of 7.6 - 7.7 g/cm³ | Typical for Martensitic Stainless Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation A50 | 20.0 °C | 0 - 17 % Show Material materials with Elongation A50 of 0 - 17 % | |
Hardness, Brinell | 20.0 °C | 0 - 235 [-] Show Material materials with Hardness, Brinell of 0 - 235 [-] | |
Hardness, Rockwell C | 20.0 °C | 0 - 22 [-] Show Material materials with Hardness, Rockwell C of 0 - 22 [-] | |
Poisson's ratio | 20.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Martensitic Stainless Steel |
Reduction of area | 20.0 °C | 0 - 35 % Show Material materials with Reduction of area of 0 - 35 % | |
Tensile strength | 20.0 °C | 0 - 690 MPa Show Material materials with Tensile strength of 0 - 690 MPa | |
Yield Strength Rp0.2, short transverse | 20.0 °C | 0 - 515 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 0 - 515 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 20.0 °C | 1E-5 - 1.5E-5 1/K Show Material materials with Coefficient of thermal expansion of 1E-5 - 1.5E-5 1/K | Typical for Martensitic Stainless Steel |
Melting point | 1375 - 1450 °C Show Material materials with Melting point of 1375 - 1450 °C | Typical for Martensitic Stainless Steel | |
Thermal conductivity | 20.0 °C | 14 - 31 W/(m·K) Show Material materials with Thermal conductivity of 14 - 31 W/(m·K) | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0 - 0.15 % Show Material materials with Carbon of 0 - 0.15 % |
Copper | 0 - 0.1 % Show Material materials with Copper of 0 - 0.1 % |
Manganese | 0 - 1 % Show Material materials with Manganese of 0 - 1 % |
Molybdenum | 0 - 0.5 % Show Material materials with Molybdenum of 0 - 0.5 % |
Nickel | 0 - 0.05 % Show Material materials with Nickel of 0 - 0.05 % |
Phosphorus | 0 - 0.04 % Show Material materials with Phosphorus of 0 - 0.04 % |
Silicon | 0 - 1.5 % Show Material materials with Silicon of 0 - 1.5 % |
Sulfur | 0 - 0.035 % Show Material materials with Sulfur of 0 - 0.035 % |