Titanio puro
DIN 17850 Grade Ti1Pd AnnealedAcero inoxidable austenítico
EN 10088-1 Grade X2CrNiMoN17-13-3 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X2CrNi19-11 solution annealed (+AT)Acero inoxidable austenítico
DIN 17440 Grade X6CrNiTi18-10 solution heat-treated and quenchedAcero inoxidable austenítico
DIN 17440 Grade X2CrNi19-11 solution heat-treated and quenchedAcero inoxidable austenítico
EN 10088-1 Grade X2CrNiMoN17-11-2 solution annealed (+AT)Acero inoxidable austenítico
DIN 17440 Grade X6CrNiMoTi17-12-2 solution heat-treated and quenchedAcero inoxidable austenítico
DIN 17440 Grade X2CrNi19-11 quenched (+Q)Acero inoxidable austenítico
EN 10272 Grade X1NiCrMoCu31-27-4 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X8CrNiNb16-13 solution annealed (+AT)Acero inoxidable austenítico
EN 10272 Grade X2CrNi18-9 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X2CrNi18-9 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X6CrNiTiB18-10 solution annealed (+AT)Acero inoxidable austenítico
EN 10216-5 Grade X6CrNiTi18-10 solution annealed (+AT)Acero inoxidable austenítico
EN 10216-5 Grade X6CrNiMoTi17-12-2 solution annealed (+AT)Acero inoxidable austenítico
EN 10216-5 Grade X8CrNiMoNb16-16 solution annealed (+AT)Acero inoxidable austenítico
EN 10216-5 Grade X8CrNiTi18-10 solution annealed (+AT)Acero inoxidable austenítico
DIN 1654-5 Grade X2CrNi19-11 quenched (+Q)