Zirconia Grinding Media Ce-Stab

Want to keep this datasheet? Save it now in your required format

Description

GNPGraystar’s Zirconia Grinding Media is the most durable and efficient meda for ball milling and attrition milling of ceramic materials. Zirconia grinding media provides a virtually contamination-free ball milling solution for a variety of industries. (Sphere roundness: 95%)

This material data has been provided by GNPGraystar Specialty Materials.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

5.95 - 6.0 g/cm³

Show Supplier Material materials with Density of 5.95 - 6.0 g/cm³

packed density: 3.6-3.8

Water absorption

0 %

Show Supplier Material materials with Water absorption of 0 %

Mechanical

PropertyValueComment

Hardness, Mohs

9.0 [-]

Show Supplier Material materials with Hardness, Mohs of 9.0 [-]

Nominal breaking force

490.0 N

Show Supplier Material materials with Nominal breaking force of 490.0 N

min., crushing load

Chemical properties

PropertyValueComment

Zirconium

95 %

Show Supplier Material materials with Zirconium of 95 %

ZrO₂+CeO₂

Technological properties

Property
Application areas

GNPGraystar’s Zirconia Grinding Media is used for audio/video recording tapes, electronic-grade ceramics, ferroelectric, piezoelectric, dielectric, capacitors, sensors, inks, dyes, paint, and other pigments.

Color

Gold

Other

Available Sizes:


Ceria Stabilized Spheres:

Φ0.4, Φ0.5, Φ0.8, Φ1, Φ1.5, Φ2, Φ2.5, Φ3, Φ4, Φ5, Φ7, Φ8, Φ10, Φ12, Φ15, Φ20, Φ25, Φ30 mm

Wear resistance

Wear Rate (normal): <0.3% , (extreme): <2%